Prestripping Protocol for Reconciling Lithium Dissolution and Galvanic Corrosion in Anode-Free Batteries

The practical viability of high-energy-density anode-free lithium metal batteries is limited by the poor reversibility of lithium plating and stripping. Low-current stripping suppresses pitting and inactive Li formation but prolongs electrolyte exposure and galvanic corrosion, whereas high-current stripping shortens the corrosion time but promotes localized dissolution and structural disintegration. Here, we introduce a pre-stripping protocol consisting of a brief low-current stripping step followed immediately by higher-current bulk stripping, thereby establishing a uniform initial dissolution front while limiting the duration of Li–Cu galvanic coupling. Measurements across representative electrolyte formulations identify three factors associated with the balance between morphological regulation and corrosion loss: nascent solid electrolyte interphase (SEI) passivation, longer-term corrosion tolerance, and dynamic reaction area evolution. In strongly passivating formulations, the morphological benefit of prestripping outweighs the additional corrosion loss and improves Li reversibility. The protocol was further evaluated in 1 Ah anode-free pouch cells, supporting its applicability to practical cell configurations.

Authors

Institutions

Publication Details

Journal
ACS Energy Letters
Published
2026-11-23
DOI
https://doi.org/10.1021/acsenergylett.6c02416
Primary Topic
Solid Electrolytes, Lithium-Metal and Lithium-Sulfur Batteries
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Prestripping Protocol for Reconciling Lithium Dissolution and Galvanic Corrosion in Anode-Free Batteries

Tianyang Yu, Teng Zhao, Li Li, Renjie Chen et al.
ACS Energy Letters
Solid Electrolytes, Lithium-Metal and Lithium-Sulfur Batteries
article

Prestripping Protocol for Reconciling Lithium Dissolution and Galvanic Corrosion in Anode-Free Batteries

Tianyang Yu, Teng Zhao, Li Li, Renjie Chen, Wangming Tang, Xue Pang, Ke Wang
article en

Abstract

The practical viability of high-energy-density anode-free lithium metal batteries is limited by the poor reversibility of lithium plating and stripping. Low-current stripping suppresses pitting and inactive Li formation but prolongs electrolyte exposure and galvanic corrosion, whereas high-current stripping shortens the corrosion time but promotes localized dissolution and structural disintegration. Here, we introduce a pre-stripping protocol consisting of a brief low-current stripping step followed immediately by higher-current bulk stripping, thereby establishing a uniform initial dissolution front while limiting the duration of Li–Cu galvanic coupling. Measurements across representative electrolyte formulations identify three factors associated with the balance between morphological regulation and corrosion loss: nascent solid electrolyte interphase (SEI) passivation, longer-term corrosion tolerance, and dynamic reaction area evolution. In strongly passivating formulations, the morphological benefit of prestripping outweighs the additional corrosion loss and improves Li reversibility. The protocol was further evaluated in 1 Ah anode-free pouch cells, supporting its applicability to practical cell configurations.

ACS Energy Letters
Beijing Institute of Technology (CN), Jinan Institute of Quantum Technology (CN)
Solid Electrolytes, Lithium-Metal and Lithium-Sulfur Batteries
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines