Ignition mechanism of plasma potential drop and double layer formation in BP-HiPIMS discharge
The formation of the double layer (DL) near the target in bipolar-pulse high-power impulse magnetron sputtering (BP-HiPIMS) is of great concern as it influences the energy of deposited ions. In this work, to understand the DL formation mechanism and its effects on ion energy, the spatial distribution and temporal evolution of the plasma potential (Vpl) have been comprehensively investigated across various target materials and discharge parameters, using a space-resolved emissive probe and a mass spectrometer. Measurements revealed that the evolution of Vpl exhibits three distinct stages: an initial overshoot followed by a platform (Stage 1), a potential drop and rise again sustained for tens of microseconds (Stage 2), and another platform until the end of the positive pulse (Stage 3). The duration of Stage 1 is related to the plasma density decay rate, which is shortened in the case of lower plasma density, higher potential gradient at the boundaries and lower atomic mass of light metals. Two distinct types of DL formation processes could be detected during Stage 2. For the first type, the DL transitions from an electron sheath in Stage 1 into anode glow at the start of Stage 2, and eventually forms a stable DL by the end of Stage 2. By contrast, for the second type, the DL is formed by a potential well near the magnetic null point. The difference between these two types may be related to both the density and ionization energy of metal atoms rather than gas atoms. Stage 3 corresponds to the self-sustained anode discharge with ionization of background gas atoms. For example, in the case of Ag target, the potential drop across the DL boundary is 18–21 V during Stage 3, a value that is slightly higher than the ionization energy of the gas. Additionally, the formation of the DL can enhance the population of high-energy ions for both metal and gas species as measured by the ion energy distribution function. Consequently, the positive pulse parameters must be carefully optimized to improve coating quality by balancing the contribution of metal ion energy against the potential detrimental effects of excessive gas ion bombardment.
Authors
- Ye Xu (ORCID: https://orcid.org/0000-0003-4322-244X)
- Mingxuan Yang (ORCID: https://orcid.org/0000-0002-1111-4076)
- Mingyue Han (ORCID: https://orcid.org/0000-0002-2420-7570)
- Yang Luo (ORCID: https://orcid.org/0009-0000-3645-3632)
- Liuhe Li (ORCID: https://orcid.org/0000-0002-6339-9835)
- WU Yiyan
- Huanjun Xie
Institutions
- Beihang University (CN)
Publication Details
- Journal
- Plasma Sources Science and Technology
- Published
- 2026-11-23
- DOI
- https://doi.org/10.1088/1361-6595/aec58c
- Primary Topic
- Low-Pressure Plasma Processing and Diagnostics
- Type
- article
- Field-Weighted Citation Impact
- 0.00