The influence of process parameter regulation and improved aging heat treatment on the quality of laser deposition repair of GH4738 turbine blades

GH4738 superalloy turbine blades easily fail under extreme service conditions. To improve remanufacturability and avoid exclusive reliance on homologous repair materials, GH4169 powder was adopted for laser deposition repair (LDR). A line energy density window of 100–150 J/mm was determined to suppress pores and cracks at the GH4169/GH4738 interface and form sound metallurgical bonding. An improved aging heat treatment (IAHT) was further used to tailor metastable microstructures in the deposited region. IAHT facilitates γ′/γ″ precipitation, partially dissolves brittle Laves phase, and converts some columnar grains into equiaxed grains. After IAHT, macroscopic residual stresses in the substrate, interface and repair zone drop by 34.55%, 46.82% and 42.57%, while intragranular micro-strain (GOS) decreases by 20.95%, 24.88% and 30.62%. The microhardness of the repair zone rises from 247.26 HV0.2 to 443.61 HV0.2. This integrated route enables high-performance blade repair using non-homologous feedstock.

Authors

Institutions

Publication Details

Journal
Materials and Manufacturing Processes
Published
2026-11-23
DOI
https://doi.org/10.1080/10426914.2026.2767839
Primary Topic
Additive Manufacturing Materials and Processes
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

The influence of process parameter regulation and improved aging heat treatment on the quality of laser deposition repair of GH4738 turbine blades

Siwei Xin, Peng Liu, Defu Liu
Materials and Manufacturing Processes
Additive Manufacturing Materials and Processes
article

The influence of process parameter regulation and improved aging heat treatment on the quality of laser deposition repair of GH4738 turbine blades

Siwei Xin, Peng Liu, Defu Liu
article en

Abstract

GH4738 superalloy turbine blades easily fail under extreme service conditions. To improve remanufacturability and avoid exclusive reliance on homologous repair materials, GH4169 powder was adopted for laser deposition repair (LDR). A line energy density window of 100–150 J/mm was determined to suppress pores and cracks at the GH4169/GH4738 interface and form sound metallurgical bonding. An improved aging heat treatment (IAHT) was further used to tailor metastable microstructures in the deposited region. IAHT facilitates γ′/γ″ precipitation, partially dissolves brittle Laves phase, and converts some columnar grains into equiaxed grains. After IAHT, macroscopic residual stresses in the substrate, interface and repair zone drop by 34.55%, 46.82% and 42.57%, while intragranular micro-strain (GOS) decreases by 20.95%, 24.88% and 30.62%. The microhardness of the repair zone rises from 247.26 HV0.2 to 443.61 HV0.2. This integrated route enables high-performance blade repair using non-homologous feedstock.

Materials and Manufacturing Processes
Central South University (CN), Shanghai Jiao Tong University (CN)
National Natural Science Foundation of China
Additive Manufacturing Materials and Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
The influence of process parameter regulation and improved aging heat treatment on the quality of laser deposition repair of GH4738 turbine blades — Siwei Xin, Peng Liu, et al. · Materials and Manufacturing Processes (2026) | TGRS Research Map | TGRS