Effect of Pack Boriding on the Surface, Wear, Corrosion, and Mechanical Properties of AISI 4140 Steel

AISI 4140 steel was pack‐borided using a powder mixture containing 70 wt.% SiC, 20 wt.% B 4 C, and 10 wt.% KBF 4 under six conditions: 900 and 950 °C for 2, 3, and 4 h. The untreated steel was designated S0. Cross‐sectional SEM observations revealed a dense surface‐modified layer with a characteristic saw‐tooth morphology consistent with boride layers reported for pack‐borided low‐alloy steels. The average layer thickness increased from 75 µm for S1 to 152 µm for S6, showing that temperature had a stronger influence on layer growth than holding time. Near‐surface microhardness values ranged from 1250 to 1476 HV0.01 and gradually decreased toward the substrate. Dry reciprocating sliding tests indicated that boriding modified the friction regime and stability rather than consistently reducing the friction coefficient. Electrochemical polarization tests in 0.1 M NaCl showed that the corrosion current density decreased from 6.059 µA cm −2 for S0 to 2.356–3.640 µA cm −2 for the borided specimens, with S2 showing the lowest value. Hot tensile tests at 300 °C revealed reductions in yield and ultimate tensile strength, whereas bending load and Charpy impact energy increased under several conditions. S3 exhibited the highest bending load and impact energy.

Authors

Institutions

Publication Details

Journal
steel research international
Published
2026-11-23
DOI
https://doi.org/10.1002/srin.70816
Primary Topic
Surface Treatment and Coatings
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effect of Pack Boriding on the Surface, Wear, Corrosion, and Mechanical Properties of AISI 4140 Steel

Özgür Tekaslan, Ali Arı
steel research international
Surface Treatment and Coatings
article

Effect of Pack Boriding on the Surface, Wear, Corrosion, and Mechanical Properties of AISI 4140 Steel

Özgür Tekaslan, Ali Arı
article en

Abstract

AISI 4140 steel was pack‐borided using a powder mixture containing 70 wt.% SiC, 20 wt.% B 4 C, and 10 wt.% KBF 4 under six conditions: 900 and 950 °C for 2, 3, and 4 h. The untreated steel was designated S0. Cross‐sectional SEM observations revealed a dense surface‐modified layer with a characteristic saw‐tooth morphology consistent with boride layers reported for pack‐borided low‐alloy steels. The average layer thickness increased from 75 µm for S1 to 152 µm for S6, showing that temperature had a stronger influence on layer growth than holding time. Near‐surface microhardness values ranged from 1250 to 1476 HV0.01 and gradually decreased toward the substrate. Dry reciprocating sliding tests indicated that boriding modified the friction regime and stability rather than consistently reducing the friction coefficient. Electrochemical polarization tests in 0.1 M NaCl showed that the corrosion current density decreased from 6.059 µA cm −2 for S0 to 2.356–3.640 µA cm −2 for the borided specimens, with S2 showing the lowest value. Hot tensile tests at 300 °C revealed reductions in yield and ultimate tensile strength, whereas bending load and Charpy impact energy increased under several conditions. S3 exhibited the highest bending load and impact energy.

steel research international
Ostim Technical University (TR)
Surface Treatment and Coatings
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.