Evaluation of Self-Healing and Microstructure of Nano-Silica Engineered Cementitious Composites Reinforced with Glass Fiber

This experimental work has investigated the effect of adding nano-silica (NS) at percentages of (1.5, 2.0, 2.5)% by weight of the total cementitious binder (CB) as a replacement on the self-healing and microstructure of engineered cementitious composites (ECC). A flow table test was conducted for fresh properties evaluation, and physical tests including density, porosity, and absorption were carried out. Besides that, mechanical tests were conducted, involving compression, flexural, and direct tension tests. Also, self-healing was evaluated by pre-cracking (50 × 50 × 50) mm cube specimens using a concentrated load under uniaxial compression, forming cracks with maximum widths ranging between 0.40 and 0.63 mm. Tests were conducted, including crack width measurement and closure monitoring over time, measurement of electrical resistivity change during the healing process, and measurement of compressive strength after 28 days under different types of curing conditions, namely moisture curing and carbonation curing. X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy-dispersive X-ray (EDX) were performed for microstructural analysis for the REF mix and NS2.0 for both wet- and carbonation-cured specimens. The results show improvement in compressive, flexural, and direct tension strength for smart ECC containing nano-silica at 2.0%. The results revealed that the best average compressive strength of pre-cracked specimens under wet curing conditions was obtained from a mix containing 2% nano-silica, at 35.8 MPa. The best average compressive strength of pre-cracked specimens under carbonation curing conditions was obtained from a mix containing 2.0% nano-silica with 1% glass fiber, at 47.96 MPa. The best crack closure rate was obtained from the 2.0% NS mixture under wet curing conditions, with the maximum sealed crack width of 0.47 mm. Also, the highest compressive strength improvement (25.44%) and direct tensile strength improvement (45.18%) were obtained from the 2.0% NS mixture; the flexural strength improvement (87.19%) was obtained from the 2.5% NS mixture.

Authors

Institutions

Publication Details

Journal
Eng—Advances in Engineering
Published
2026-11-23
DOI
https://doi.org/10.3390/eng7120666
Primary Topic
Microbial Applications in Construction Materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Evaluation of Self-Healing and Microstructure of Nano-Silica Engineered Cementitious Composites Reinforced with Glass Fiber

Hussein H. Zghair, Mohammad A. Haseeb
Eng—Advances in Engineering
Microbial Applications in Construction Materials
article

Evaluation of Self-Healing and Microstructure of Nano-Silica Engineered Cementitious Composites Reinforced with Glass Fiber

Hussein H. Zghair, Mohammad A. Haseeb
article en

Abstract

This experimental work has investigated the effect of adding nano-silica (NS) at percentages of (1.5, 2.0, 2.5)% by weight of the total cementitious binder (CB) as a replacement on the self-healing and microstructure of engineered cementitious composites (ECC). A flow table test was conducted for fresh properties evaluation, and physical tests including density, porosity, and absorption were carried out. Besides that, mechanical tests were conducted, involving compression, flexural, and direct tension tests. Also, self-healing was evaluated by pre-cracking (50 × 50 × 50) mm cube specimens using a concentrated load under uniaxial compression, forming cracks with maximum widths ranging between 0.40 and 0.63 mm. Tests were conducted, including crack width measurement and closure monitoring over time, measurement of electrical resistivity change during the healing process, and measurement of compressive strength after 28 days under different types of curing conditions, namely moisture curing and carbonation curing. X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy-dispersive X-ray (EDX) were performed for microstructural analysis for the REF mix and NS2.0 for both wet- and carbonation-cured specimens. The results show improvement in compressive, flexural, and direct tension strength for smart ECC containing nano-silica at 2.0%. The results revealed that the best average compressive strength of pre-cracked specimens under wet curing conditions was obtained from a mix containing 2% nano-silica, at 35.8 MPa. The best average compressive strength of pre-cracked specimens under carbonation curing conditions was obtained from a mix containing 2.0% nano-silica with 1% glass fiber, at 47.96 MPa. The best crack closure rate was obtained from the 2.0% NS mixture under wet curing conditions, with the maximum sealed crack width of 0.47 mm. Also, the highest compressive strength improvement (25.44%) and direct tensile strength improvement (45.18%) were obtained from the 2.0% NS mixture; the flexural strength improvement (87.19%) was obtained from the 2.5% NS mixture.

Eng—Advances in EngineeringVol. 7(12)
University of Technology - Iraq (IQ)
Microbial Applications in Construction Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon