Investigating the Effect of Metakaolin on the Flow, Compressive Strength and Water Absorption of High Performance Concrete
High performance concrete (HPC) requires high binder contents, thereby increasing cost and CO₂ emissions. Metakaolin (MK) from locally available kaolin is a promising partial cement replacement, but its interaction with superplasticiser, water-cement ratio and aggregate-cement proportions in Portland-limestone cement HPC has not been fully investigated. This study examined the combined effect of five mix variables on the fresh, mechanical and durability properties of MK-HPC and identified mixes balancing flow, strength and impermeability. A five-factor, five-level central composite design (60 runs) varied MK (5-15% cement replacement), PCE superplasticiser (1.00-1.20%), water-cement ratio (0.31-0.35), coarse to fine aggregate ratio (0.60-1.00) and cement to fine aggregate ratio (1.10-1.50), using cement and metakaolin. Slump flow, 28-day compressive strength and water absorption of HPC were determined. The results revealed that slump flow ranged from 665 to 730 mm, placing every mix within EFNARC class SF2. Compressive strength ranged from 20.9 to 55.3 MPa, while water absorption value ranges from 0.09-1.17%. Concrete specimen that had 28 days compressive strength above 55 N/mm² was achieved by mixes containing (MK= 10-12.5%, SP = 1.1-1.15%, W/C = 0.32-0.33, CA = 0.9-1.0, CE = 1.3-1.4).
Authors
- Mohammed Abdulmumin Nda
- Abdulmumin Ahmed Shuaibu
- Ahmad Alkali Kakashehu
Institutions
- Baze University (NG)
Publication Details
- Journal
- Iconic Research and Engineering Journals
- Published
- 2026-11-23
- DOI
- https://doi.org/10.64388/ire1725546
- Primary Topic
- Concrete and Cement Materials Research
- Type
- article
- Field-Weighted Citation Impact
- 0.00