Enhanced Self-Healing Efficiency and Long-Term Bacterial Viability in Sustainable Concrete Using Immobilized Bacillus Subtilis in Porous Biochar Carriers

The global demand for Portland cement concrete continues to rise, contributing approximately 7% of total anthropogenic CO2 emissions. Extending the service life of reinforced concrete structures through autonomous crack repair offers a sustainable solution to reduce maintenance costs and environmental impact. Previous studies have demonstrated that direct incorporation of alkali-resistant Bacillus spores into cement paste results in high early-age crack-healing potential; however, bacterial viability drops significantly after 4 months due to pore-size refinement below 1 µm during cement hydration. To overcome this limitation, this study investigates the immobilization of Bacillus subtilis spores along with calcium lactate within porous agricultural-waste biochar as a protective carrier. Concrete specimens (M30 grade) were prepared with varying dosages of immobilized bacterial carriers (0%, 5%, 10%, and 15% by weight of fine aggregate). Mechanical properties (compressive and split tensile strength), crack-healing efficiency at 28, 90, and 180 days, and water permeability were evaluated. Experimental results demonstrate that the incorporation of 10% immobilized bacterial biochar increased 28-day compressive strength by 12.4% compared to the control mix and achieved complete autonomous healing of cracks up to 0.45 mm width even after 180 days. Microstructural characterization via Scanning Electron Microscopy (SEM) and X-Ray Diffraction (XRD) confirmed dense precipitation of calcite (CaCO3) crystals within the crack matrix. This approach provides an eco-friendly, cost-effective pathway for durable, self-healing structural concrete.

Authors

Publication Details

Journal
International Journal of Science and Engineering Science Research
Published
2026-11-22
DOI
https://doi.org/10.63671/ijsesr.v2i4.192
Primary Topic
Microbial Applications in Construction Materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Enhanced Self-Healing Efficiency and Long-Term Bacterial Viability in Sustainable Concrete Using Immobilized Bacillus Subtilis in Porous Biochar Carriers

Deepak Sonkar, Kirti Bhatt, Bikash Mandal, Himanshu Tripathi et al.
International Journal of Science and Engineering Science Research
Microbial Applications in Construction Materials
article

Enhanced Self-Healing Efficiency and Long-Term Bacterial Viability in Sustainable Concrete Using Immobilized Bacillus Subtilis in Porous Biochar Carriers

Deepak Sonkar, Kirti Bhatt, Bikash Mandal, Himanshu Tripathi, Mahima
article en

Abstract

The global demand for Portland cement concrete continues to rise, contributing approximately 7% of total anthropogenic CO2 emissions. Extending the service life of reinforced concrete structures through autonomous crack repair offers a sustainable solution to reduce maintenance costs and environmental impact. Previous studies have demonstrated that direct incorporation of alkali-resistant Bacillus spores into cement paste results in high early-age crack-healing potential; however, bacterial viability drops significantly after 4 months due to pore-size refinement below 1 µm during cement hydration. To overcome this limitation, this study investigates the immobilization of Bacillus subtilis spores along with calcium lactate within porous agricultural-waste biochar as a protective carrier. Concrete specimens (M30 grade) were prepared with varying dosages of immobilized bacterial carriers (0%, 5%, 10%, and 15% by weight of fine aggregate). Mechanical properties (compressive and split tensile strength), crack-healing efficiency at 28, 90, and 180 days, and water permeability were evaluated. Experimental results demonstrate that the incorporation of 10% immobilized bacterial biochar increased 28-day compressive strength by 12.4% compared to the control mix and achieved complete autonomous healing of cracks up to 0.45 mm width even after 180 days. Microstructural characterization via Scanning Electron Microscopy (SEM) and X-Ray Diffraction (XRD) confirmed dense precipitation of calcite (CaCO3) crystals within the crack matrix. This approach provides an eco-friendly, cost-effective pathway for durable, self-healing structural concrete.

International Journal of Science and Engineering Science ResearchVol. 2(4)
Microbial Applications in Construction Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
Enhanced Self-Healing Efficiency and Long-Term Bacterial Viability in Sustainable Concrete Using Immobilized Bacillus Subtilis in Porous Biochar Carriers — Deepak Sonkar, Kirti Bhatt, et al. · International Journal of Science and Engineering Science Research (2026) | TGRS Research Map | TGRS