Performance Evaluation of Recycled Aggregate Concrete Through Ternary Modification with Metakaolin, Silica Fume, and Polypropylene Fibers

Recycled aggregate concrete (RAC) offers significant environmental benefits but is often limited by high porosity, weak interfacial transition zones, and reduced mechanical and durability performance. This study evaluated the long-term effects of metakaolin (15%), an aluminosilicate mineral derived from kaolin clay, silica fume (7.5%), a metallurgical by-product of silicon and ferrosilicon smelting and polypropylene fibers (PPFs, 0–1.5%) on RAC containing 0%, 50%, 75%, and 100% recycled coarse aggregate (RA), a mineral residue stream from construction and demolition waste. Sixteen concrete mixtures were produced, and 768 cylindrical specimens were tested for slump, compressive strength, split tensile strength, water absorption, sulfuric acid resistance, ultrasonic pulse velocity, rebound number, and microstructural characteristics up to 180 days. Increasing RA and PPF contents reduced workability, with slump decreasing from 98 mm to 40 mm. The mixture containing 1% PPF and 0% RA achieved the highest 180-day compressive and split tensile strengths of 64.4 MPa and 6.9 MPa, respectively, while the corresponding 50% RA mixture attained 46.6 MPa and 5.1 MPa. Under sulfuric acid exposure, 1.5% PPF reduced the 180-day mass loss of the 50% RA mixture from 23% to 14%. SEM and nondestructive tests confirmed improved matrix densification, interfacial bonding, and crack bridging. Overall, 1% PPF with 50% RA provided the best balance between strength, durability, and sustainability for structural concrete applications. The enhanced sulfuric acid resistance is particularly beneficial for mining and mineral processing infrastructure exposed to aggressive acidic environments, such as acid mine drainage, sulfide-rich tailings, and metallurgical plant floors

Authors

Institutions

Publication Details

Journal
Journal of Natural Fibers
Published
2026-11-20
DOI
https://doi.org/10.1080/15440478.2026.2758991
Primary Topic
Recycled Aggregate Concrete Performance
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Performance Evaluation of Recycled Aggregate Concrete Through Ternary Modification with Metakaolin, Silica Fume, and Polypropylene Fibers

Ali Ajwad, George Uwadiegwu Alaneme, Ahmed A. Alawi Al-Naghi, Khaled Mohamed Elhadi et al.
Journal of Natural Fibers
Recycled Aggregate Concrete Performance
article

Performance Evaluation of Recycled Aggregate Concrete Through Ternary Modification with Metakaolin, Silica Fume, and Polypropylene Fibers

Ali Ajwad, George Uwadiegwu Alaneme, Ahmed A. Alawi Al-Naghi, Khaled Mohamed Elhadi, Muhammad Sarmad Mahmood, Nejib Ghazouani, Muhammad Zeeshan Qureshi, Tariq Ali
article en

Abstract

Recycled aggregate concrete (RAC) offers significant environmental benefits but is often limited by high porosity, weak interfacial transition zones, and reduced mechanical and durability performance. This study evaluated the long-term effects of metakaolin (15%), an aluminosilicate mineral derived from kaolin clay, silica fume (7.5%), a metallurgical by-product of silicon and ferrosilicon smelting and polypropylene fibers (PPFs, 0–1.5%) on RAC containing 0%, 50%, 75%, and 100% recycled coarse aggregate (RA), a mineral residue stream from construction and demolition waste. Sixteen concrete mixtures were produced, and 768 cylindrical specimens were tested for slump, compressive strength, split tensile strength, water absorption, sulfuric acid resistance, ultrasonic pulse velocity, rebound number, and microstructural characteristics up to 180 days. Increasing RA and PPF contents reduced workability, with slump decreasing from 98 mm to 40 mm. The mixture containing 1% PPF and 0% RA achieved the highest 180-day compressive and split tensile strengths of 64.4 MPa and 6.9 MPa, respectively, while the corresponding 50% RA mixture attained 46.6 MPa and 5.1 MPa. Under sulfuric acid exposure, 1.5% PPF reduced the 180-day mass loss of the 50% RA mixture from 23% to 14%. SEM and nondestructive tests confirmed improved matrix densification, interfacial bonding, and crack bridging. Overall, 1% PPF with 50% RA provided the best balance between strength, durability, and sustainability for structural concrete applications. The enhanced sulfuric acid resistance is particularly beneficial for mining and mineral processing infrastructure exposed to aggressive acidic environments, such as acid mine drainage, sulfide-rich tailings, and metallurgical plant floors

Journal of Natural FibersVol. 23(1)
Northern Border University (SA), University of South Africa (ZA), University of Engineering and Technology Taxila (PK), Kampala International University (UG), University of Ha'il (SA), King Khalid University (SA), University of Management and Technology (PK)
Recycled Aggregate Concrete Performance
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon