Long-term bond degradation of glass and basalt FRP reinforcement in high pH alkali-activated concrete (AAC)

This study investigates the long-term bond durability and multi-scale degradation mechanisms of glass fibre-reinforced polymer (GFRP) and basalt fibre-reinforced polymer (BFRP) bars embedded in a high pH alkali-activated concrete (AAC) matrix. Long-term bond performance was evaluated after AAC embedment for up to 720 days at 20°C. Accelerated ageing at 60°C was performed on bare GFRP bars for 7, 30 and 90 days before casting, as BFRP bars disintegrated within three days under these conditions preventing further testing. Material degradation was assessed using interlaminar shear strength (ILSS), Fourier transform infrared (FTIR) spectroscopy and scanning electron microscopy (SEM), while structural bond performance was evaluated through pull-out testing. The bisphenol-A vinyl-ester GFRP exhibited high hydrolytic resistance, retaining more than 89% of its ILSS and maintaining its initial pull-out capacity after two years of natural exposure. In contrast, the epoxy-based BFRP showed pronounced alkaline degradation, with FTIR and SEM indicating ester hydrolysis, matrix cracking and fibre–matrix interfacial deterioration. This was accompanied by a 70% reduction in ILSS and a 33% loss in pull-out capacity, with a shift towards premature bar rupture. The bond-slip responses were further evaluated using four analytical models. The suggested modified two-part Popovics model provided the most accurate representation of the bond stress-slip response and most closely reproduced the experimental pre- and post-peak fracture energies compared to mBPE, CMR, and Rolland-CZM analytical models. Overall, the results highlight the importance of hydrolytic stability in FRP–AAC durability and the value of integrating multi-scale degradation assessment with bond stress–slip modelling.

Authors

Institutions

Publication Details

Journal
Construction and Building Materials
Published
2026-11-21
DOI
https://doi.org/10.1016/j.conbuildmat.2026.148930
Primary Topic
Structural Behavior of Reinforced Concrete
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Long-term bond degradation of glass and basalt FRP reinforcement in high pH alkali-activated concrete (AAC)

Eleni Toumpanaki, Asaad Biqai, Ian Hamerton, Manjola Caro
Construction and Building Materials
Structural Behavior of Reinforced Concrete
article

Long-term bond degradation of glass and basalt FRP reinforcement in high pH alkali-activated concrete (AAC)

Eleni Toumpanaki, Asaad Biqai, Ian Hamerton, Manjola Caro
article en

Abstract

This study investigates the long-term bond durability and multi-scale degradation mechanisms of glass fibre-reinforced polymer (GFRP) and basalt fibre-reinforced polymer (BFRP) bars embedded in a high pH alkali-activated concrete (AAC) matrix. Long-term bond performance was evaluated after AAC embedment for up to 720 days at 20°C. Accelerated ageing at 60°C was performed on bare GFRP bars for 7, 30 and 90 days before casting, as BFRP bars disintegrated within three days under these conditions preventing further testing. Material degradation was assessed using interlaminar shear strength (ILSS), Fourier transform infrared (FTIR) spectroscopy and scanning electron microscopy (SEM), while structural bond performance was evaluated through pull-out testing. The bisphenol-A vinyl-ester GFRP exhibited high hydrolytic resistance, retaining more than 89% of its ILSS and maintaining its initial pull-out capacity after two years of natural exposure. In contrast, the epoxy-based BFRP showed pronounced alkaline degradation, with FTIR and SEM indicating ester hydrolysis, matrix cracking and fibre–matrix interfacial deterioration. This was accompanied by a 70% reduction in ILSS and a 33% loss in pull-out capacity, with a shift towards premature bar rupture. The bond-slip responses were further evaluated using four analytical models. The suggested modified two-part Popovics model provided the most accurate representation of the bond stress-slip response and most closely reproduced the experimental pre- and post-peak fracture energies compared to mBPE, CMR, and Rolland-CZM analytical models. Overall, the results highlight the importance of hydrolytic stability in FRP–AAC durability and the value of integrating multi-scale degradation assessment with bond stress–slip modelling.

Construction and Building MaterialsVol. 551
University of Bristol (GB)
Structural Behavior of Reinforced Concrete
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines