Influence of curing conditions on macro-pore porosity and compactness of metakaolin-slag-based geopolymer mortar using X-ray computed tomography

One of the limitations of metakaolin (MK)-based two-part geopolymer (GP) mortar is the long setting time, typically 12 to 24 h or more in some formulations. This study aims to reduce the setting times and macro-pores, increase void compactness, and void sphericity of MK-based GP mortar to address this limitation. The objectives are to improve fresh properties, mechanical performance, and microstructure through slag modification and a controlled curing regime. Four mixes were developed and tested by replacing MK with slag at 5% increments up to 15%. GP mortar was excited with Na 2 SiO 3 and NaOH, and the fresh properties were characterised. Cube and beam samples were cured at an elevated temperature (ET) before climate-controlled (CC) curing, while other samples were cured at CC conditions. Samples were examined for compressive (CS), flexural (FS), and direct tensile (DTS) strengths after 7- and 28-day curing. Macro-pore characteristics and internal morphology of GP mortar samples were investigated using X-ray computed tomography (XCT) and scanning electron microscopy (SEM). Workability and setting times were reduced significantly due to the predominantly finer slag particles than MK, which increases the water demand of GP mortar. Furthermore, the larger surface area of slag (0.921 m 2 /g) than MK particles (0.838 m 2 /g) increases the chemical reactivity of the composite, thereby increasing the water demand. The CS, DTS, and FS of the ET-cured samples outperformed the CC-cured samples in all mixes by up to 23%, 39%, and 42%, respectively. The strength increase associated with slag incorporation is more pronounced at 7 days than at 28 days due to the quick early-age reaction of slag, while the pure MK catches up significantly by 28 days. XCT reveals that slag inclusion reduces macro-pore porosity in the CC- and ET-cured samples by up to 13% and 20%, respectively. SEM shows a compact internal morphology of the hydration product in ET-cured samples. Curing regime and slag inclusion reduce setting times, macro-pores and enhance the mechanical performance of GP mortar.

Authors

Institutions

Publication Details

Journal
Discover Materials
Published
2026-11-21
DOI
https://doi.org/10.1007/s43939-026-01073-9
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Influence of curing conditions on macro-pore porosity and compactness of metakaolin-slag-based geopolymer mortar using X-ray computed tomography

Adewumi John Babafemi, Mustapha Bamidele Jaji
Discover Materials
Concrete and Cement Materials Research
article

Influence of curing conditions on macro-pore porosity and compactness of metakaolin-slag-based geopolymer mortar using X-ray computed tomography

Adewumi John Babafemi, Mustapha Bamidele Jaji
article en

Abstract

One of the limitations of metakaolin (MK)-based two-part geopolymer (GP) mortar is the long setting time, typically 12 to 24 h or more in some formulations. This study aims to reduce the setting times and macro-pores, increase void compactness, and void sphericity of MK-based GP mortar to address this limitation. The objectives are to improve fresh properties, mechanical performance, and microstructure through slag modification and a controlled curing regime. Four mixes were developed and tested by replacing MK with slag at 5% increments up to 15%. GP mortar was excited with Na 2 SiO 3 and NaOH, and the fresh properties were characterised. Cube and beam samples were cured at an elevated temperature (ET) before climate-controlled (CC) curing, while other samples were cured at CC conditions. Samples were examined for compressive (CS), flexural (FS), and direct tensile (DTS) strengths after 7- and 28-day curing. Macro-pore characteristics and internal morphology of GP mortar samples were investigated using X-ray computed tomography (XCT) and scanning electron microscopy (SEM). Workability and setting times were reduced significantly due to the predominantly finer slag particles than MK, which increases the water demand of GP mortar. Furthermore, the larger surface area of slag (0.921 m 2 /g) than MK particles (0.838 m 2 /g) increases the chemical reactivity of the composite, thereby increasing the water demand. The CS, DTS, and FS of the ET-cured samples outperformed the CC-cured samples in all mixes by up to 23%, 39%, and 42%, respectively. The strength increase associated with slag incorporation is more pronounced at 7 days than at 28 days due to the quick early-age reaction of slag, while the pure MK catches up significantly by 28 days. XCT reveals that slag inclusion reduces macro-pore porosity in the CC- and ET-cured samples by up to 13% and 20%, respectively. SEM shows a compact internal morphology of the hydration product in ET-cured samples. Curing regime and slag inclusion reduce setting times, macro-pores and enhance the mechanical performance of GP mortar.

Discover Materials
Stellenbosch University (ZA), University of KwaZulu-Natal (ZA)
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon