Influence of Pack Boronizing Process Parameters on the Microstructure, Tribological Performance, Corrosion Resistance, and Mechanical Properties of H13 Tool Steel
In this study, AISI H13 hot-work tool steel is pack boronized at 900 and 950°C for 2–4 h using a 70% SiC-20% B 4 C-10% KBF 4 powder mixture. Cross-sectional SEM-EDS analyses show a continuous saw-tooth boride layer with a strong boron gradient. The layer thickness ranges from 22 to 50 µm; at 900°C it rises from 24.5 to 45.5 µm when the duration increases from 2 to 4 h (85.7%), while at 950°C it increases from 31.5 to 50 µm (58.7%). At constant duration, raising the temperature from 900°C to 950°C increases thickness by 28.6% at 2 h but only 9.9% at 4 h, indicating diffusion-rate dominance at shorter times and alloying-element barrier effects at longer times. Microhardness values reach 985–1460 HV0.01 at 0.05 mm and decrease gradually to 333–520 HV0.01 at 0.2 mm. Dry sliding tests show a 13.8%–30% reduction in friction relative to the reference (μ avg = 0.80). Tribocorrosion tests reveal a drop in I corr from 22.720 to 1.756–6.323, with the lowest value at 900°C–4 h. Tensile tests at 300°C show significant increases in yield (577 → 987–1366 MPa) and ultimate strength (614 → 1123–1765 MPa), while Charpy impact energy decreases markedly. The results highlight the need to balance boride layer growth with brittleness.
Authors
- Özgür Tekaslan
- Ali Arı (ORCID: https://orcid.org/0000-0003-2702-2982)
Institutions
- Ostim Technical University (TR)
Publication Details
- Journal
- Proceedings of the Institution of Mechanical Engineers Part C Journal of Mechanical Engineering Science
- Published
- 2026-11-20
- DOI
- https://doi.org/10.1177/09544062261501703
- Primary Topic
- Surface Treatment and Coatings
- Type
- article
- Field-Weighted Citation Impact
- 0.00