From cryogenic ball milling to aqueous dispersion: preparation of fragment-like polyethylene and polystyrene microplastic test materials

Preparation of reproducible microplastic (MP) test materials remains a key challenge in fate, toxicity, and removal studies. This study developed a facile cryogenic ball-milling and surfactant-assisted dispersion workflow to produce fragment-like polyethylene (PE) and polystyrene (PS) MP test materials. Milling was optimised by varying feed mass, milling time, bead size, bead number, and cycle configuration. The lowest PS Dv 90 was 244 µm, achieved using 1-g feed, single 25-mm bead and 5 min of milling time. Optimised conditions for PE (0.25 g of feed with five 10-mm beads milled for 15 min) reduced Dv 90 from 235 to 59 µm. MPs produced under the respective optimised milling conditions were tested in 0.02% (w/v) aqueous solutions of Tween 80, Triton X-405, polyvinyl alcohol (PVA) and polyethylene glycol (PEG). Suspension behaviour was assessed by 24-h visual observation and 2-h turbidity measurements, supported by contact-angle and FTIR analyses. Among the tested surfactants, Tween 80 produced the most effective dispersion and reduced the contact angles from 115° to 84° (PE) and 88° to 57° (PS). Under static conditions, visible suspension persisted for at least 24 h for PE and more than 3 h for PS. The observed behaviour is consistent with improved interfacial wetting and possible steric stabilisation at the MP-water interface. FTIR spectra of the recovered, rinsed MPs retained the characteristic polymer bands, with no detectable chemical modification. These findings guide the selection of milling conditions and dispersing agents for preparing fragment-like MP suspensions for laboratory studies.

Authors

Institutions

Publication Details

Journal
Environmental Science and Pollution Research
Published
2026-11-21
DOI
https://doi.org/10.1007/s11356-026-38417-0
Primary Topic
Microplastics and Plastic Pollution
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

From cryogenic ball milling to aqueous dispersion: preparation of fragment-like polyethylene and polystyrene microplastic test materials

Adnan Irshad, Rehan Khalid, Veena Sahajwalla, Rasoul Khayyam Nekouei
Environmental Science and Pollution Research
Microplastics and Plastic Pollution
article

From cryogenic ball milling to aqueous dispersion: preparation of fragment-like polyethylene and polystyrene microplastic test materials

Adnan Irshad, Rehan Khalid, Veena Sahajwalla, Rasoul Khayyam Nekouei
article en

Abstract

Preparation of reproducible microplastic (MP) test materials remains a key challenge in fate, toxicity, and removal studies. This study developed a facile cryogenic ball-milling and surfactant-assisted dispersion workflow to produce fragment-like polyethylene (PE) and polystyrene (PS) MP test materials. Milling was optimised by varying feed mass, milling time, bead size, bead number, and cycle configuration. The lowest PS Dv 90 was 244 µm, achieved using 1-g feed, single 25-mm bead and 5 min of milling time. Optimised conditions for PE (0.25 g of feed with five 10-mm beads milled for 15 min) reduced Dv 90 from 235 to 59 µm. MPs produced under the respective optimised milling conditions were tested in 0.02% (w/v) aqueous solutions of Tween 80, Triton X-405, polyvinyl alcohol (PVA) and polyethylene glycol (PEG). Suspension behaviour was assessed by 24-h visual observation and 2-h turbidity measurements, supported by contact-angle and FTIR analyses. Among the tested surfactants, Tween 80 produced the most effective dispersion and reduced the contact angles from 115° to 84° (PE) and 88° to 57° (PS). Under static conditions, visible suspension persisted for at least 24 h for PE and more than 3 h for PS. The observed behaviour is consistent with improved interfacial wetting and possible steric stabilisation at the MP-water interface. FTIR spectra of the recovered, rinsed MPs retained the characteristic polymer bands, with no detectable chemical modification. These findings guide the selection of milling conditions and dispersing agents for preparing fragment-like MP suspensions for laboratory studies.

Environmental Science and Pollution Research
UNSW Sydney (AU)
Microplastics and Plastic Pollution
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
From cryogenic ball milling to aqueous dispersion: preparation of fragment-like polyethylene and polystyrene microplastic test materials — Adnan Irshad, Rehan Khalid, et al. · Environmental Science and Pollution Research (2026) | TGRS Research Map | TGRS