Multiple Synergistic Effects of Different Stretching and Heating Fields on the Structure Evolution and α′-to-α Transition of PA66 Fibers during Melt Spinning

This study prepared high-strength, low-elongation PA66 fibers (tensile strength ∼ 10.14 cN/dtex, elongation ∼ 10.5%) via high-speed one-step melt spinning combined with two-stage drawing and heat setting, achieving a maximum draw ratio exceeding 5.5. Using 2D-SAXS/WAXS and FTIR, the competitive multiscale structural evolution of PA66 fibers under thermal and tensile-stress driving was systematically investigated, covering microstructure (crystal transition, chain conformation, hydrogen bonding), submicrostructure (long period and orientation), and macroscopic mechanical properties; and a three-phase structure and crystal-transition model was established. Drawing and heat setting promoted the breaking of irregular hydrogen bonds and the reconstruction of ordered ones, accompanied by lattice deformation and trans-conformation recovery. Both L-PA66 and H-PA66 fibers exhibited an α′-to-α crystal transition; H-PA66 fibers showed a higher crystal transition temperature (ST = 250 °C) and insignificant Poisson contraction due to their high orientation and compact chain conformation. Under high stress, MAF in H-PA66 fibers gradually transformed into RAF, giving a more perfect and uniform structure with markedly enhanced orientation; fibrillar crystals grew along the (010)/(110) planes, the grains were refined, and crystallinity and mechanical properties improved significantly. L-PA66 fibers tended toward thermally controlled equilibrium relaxation due to H-DT; although the crystalline region gradually became more perfect and partially compensated for amorphous deorientation, deorientation driven by higher ST (230 °C < T < 250 °C) remained unavoidable. This study constructed a structure–property model of PA66 fibers under different drawing processes, providing a theoretical basis for high-performance polyamide fibers.

Authors

Institutions

Publication Details

Journal
ACS Applied Polymer Materials
Published
2026-11-21
DOI
https://doi.org/10.1021/acsapm.6c04325
Primary Topic
Polymer crystallization and properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Multiple Synergistic Effects of Different Stretching and Heating Fields on the Structure Evolution and α′-to-α Transition of PA66 Fibers during Melt Spinning

Ze-Tian Zhang, Yongming Shi, Weixin Wu, Bo Wang et al.
ACS Applied Polymer Materials
Polymer crystallization and properties
article

Multiple Synergistic Effects of Different Stretching and Heating Fields on the Structure Evolution and α′-to-α Transition of PA66 Fibers during Melt Spinning

Ze-Tian Zhang, Yongming Shi, Weixin Wu, Bo Wang, Shuang-You Shi, Zong-Zi Hou, Peng-Fei Wu, Xian-Ning Shi
article en

Abstract

This study prepared high-strength, low-elongation PA66 fibers (tensile strength ∼ 10.14 cN/dtex, elongation ∼ 10.5%) via high-speed one-step melt spinning combined with two-stage drawing and heat setting, achieving a maximum draw ratio exceeding 5.5. Using 2D-SAXS/WAXS and FTIR, the competitive multiscale structural evolution of PA66 fibers under thermal and tensile-stress driving was systematically investigated, covering microstructure (crystal transition, chain conformation, hydrogen bonding), submicrostructure (long period and orientation), and macroscopic mechanical properties; and a three-phase structure and crystal-transition model was established. Drawing and heat setting promoted the breaking of irregular hydrogen bonds and the reconstruction of ordered ones, accompanied by lattice deformation and trans-conformation recovery. Both L-PA66 and H-PA66 fibers exhibited an α′-to-α crystal transition; H-PA66 fibers showed a higher crystal transition temperature (ST = 250 °C) and insignificant Poisson contraction due to their high orientation and compact chain conformation. Under high stress, MAF in H-PA66 fibers gradually transformed into RAF, giving a more perfect and uniform structure with markedly enhanced orientation; fibrillar crystals grew along the (010)/(110) planes, the grains were refined, and crystallinity and mechanical properties improved significantly. L-PA66 fibers tended toward thermally controlled equilibrium relaxation due to H-DT; although the crystalline region gradually became more perfect and partially compensated for amorphous deorientation, deorientation driven by higher ST (230 °C < T < 250 °C) remained unavoidable. This study constructed a structure–property model of PA66 fibers under different drawing processes, providing a theoretical basis for high-performance polyamide fibers.

ACS Applied Polymer Materials
China Textile Academy (CN)
Polymer crystallization and properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon