Degradation Mechanisms of Concrete Following High-Temperature Exposure and Different Cooling Methods

High-temperature exposure substantially alters the physical and mechanical properties of concrete, and understanding the underlying degradation mechanisms can provide an important basis for post-fire assessment, emergency response, and repair decisions. In this study, concrete specimens were heated to ten target temperatures (200, 300, 350, 400, 450, 500, 550, 600, 700, and 800 ∘ C ) and subsequently subjected to either natural cooling or water cooling. After the specimens had cooled and dried, their surface color, mass, relative dynamic modulus of elasticity, electrical resistance, and compressive strength were measured. Surface alkalinity was assessed by observing color changes following the application of phenolphthalein, while the CIE-L * a * b * color system provided a quantitative description of changes in surface appearance. The findings indicate an association between phenolphthalein-induced surface color and the presence of Ca(OH) 2 ; more intense coloration is consistent with a stronger alkaline response, although the color alone does not directly quantify the compound’s concentration. Mass loss increased with heating temperature, principally reflecting moisture loss and subsequent thermally induced decomposition of hydration products. The development of cracking and changes in moisture state also influenced electrical resistance. With increasing temperature, resistance rose after natural cooling but declined after water cooling, indicating that the cooling procedure influenced the electrical response. Both relative dynamic modulus of elasticity and residual compressive strength decreased as exposure temperature increased, with particularly severe deterioration in the 600–800 ∘ C range. Taken together, the measured variables provide complementary indicators of post-heating damage and show why the cooling history must be considered when assessing the condition of fire-exposed concrete.

Authors

Publication Details

Journal
Archives des sciences a multidisciplinary journal
Published
2026-11-20
DOI
https://doi.org/10.68304/as/76527
Primary Topic
Fire effects on concrete materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Degradation Mechanisms of Concrete Following High-Temperature Exposure and Different Cooling Methods

Shaojun Fu, Hao Yuan
Archives des sciences a multidisciplinary journal
Fire effects on concrete materials
article

Degradation Mechanisms of Concrete Following High-Temperature Exposure and Different Cooling Methods

Shaojun Fu, Hao Yuan
article en

Abstract

High-temperature exposure substantially alters the physical and mechanical properties of concrete, and understanding the underlying degradation mechanisms can provide an important basis for post-fire assessment, emergency response, and repair decisions. In this study, concrete specimens were heated to ten target temperatures (200, 300, 350, 400, 450, 500, 550, 600, 700, and 800 ∘ C ) and subsequently subjected to either natural cooling or water cooling. After the specimens had cooled and dried, their surface color, mass, relative dynamic modulus of elasticity, electrical resistance, and compressive strength were measured. Surface alkalinity was assessed by observing color changes following the application of phenolphthalein, while the CIE-L * a * b * color system provided a quantitative description of changes in surface appearance. The findings indicate an association between phenolphthalein-induced surface color and the presence of Ca(OH) 2 ; more intense coloration is consistent with a stronger alkaline response, although the color alone does not directly quantify the compound’s concentration. Mass loss increased with heating temperature, principally reflecting moisture loss and subsequent thermally induced decomposition of hydration products. The development of cracking and changes in moisture state also influenced electrical resistance. With increasing temperature, resistance rose after natural cooling but declined after water cooling, indicating that the cooling procedure influenced the electrical response. Both relative dynamic modulus of elasticity and residual compressive strength decreased as exposure temperature increased, with particularly severe deterioration in the 600–800 ∘ C range. Taken together, the measured variables provide complementary indicators of post-heating damage and show why the cooling history must be considered when assessing the condition of fire-exposed concrete.

Archives des sciences a multidisciplinary journalVol. 76(5)
Fire effects on concrete materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon