Revealing Ti-6Al-4V process-microstructure-property relationships in high-speed annular laser directed energy deposition via in-situ monitoring

Although laser-directed energy deposition (L-DED) has been widely used owing to its high material utilization, short manufacturing cycle, and capability to fabricate large and complex components, conventional L-DED processes still face a trade-off between deposition rate and geometric accuracy, which restricts their application in areas requiring both high throughput and high precision. To address this trade-off, this work investigated off-axis powder feeding with a quasi-Gaussian laser beam and coaxial powder feeding with an annular laser beam during Ti-6Al-4V deposition at 12 and 36 mm·s −1 , aiming to clarify how the annular L-DED configuration affects process stability, deposition behavior, microstructural refinement, and mechanical properties under high-speed conditions. In-situ monitoring reveals that, under the high-speed deposition condition, the annular laser causes dominant energy absorption to shift from the substrate melt pool to the flying powder. Namely, as the scanning speed for the annular laser increases from 12 to 36 mm·s −1 , the average area and temperature of the melt pool decrease by 48.4% and 9.3%, respectively, and the spattering reduces significantly. This can be attributed to the redistribution of laser energy from the center toward the periphery by the annular beam, which improves the spatial overlap between the powder stream and laser energy, thereby forming a shallower and more stable melt pool. Thus, significant grain refinement is achieved in the deposition. In detail, microstructural analysis shows that the sample obtained using the annular laser at a high speed of 36 mm·s −1 exhibits the finest α-lath thickness (0.26±0.04 µm). Its mechanical properties follow the Hall-Petch relationship, with a tensile strength of 1,211.5 MPa, hardness of 394.8 HV 0.2 , and elongation of 7.0%. The high-speed annular L-DED process combines high efficiency, high strength, and excellent stability, providing a feasible route for additive manufacturing of advanced metallic components.

Authors

Institutions

Publication Details

Journal
China Foundry
Published
2026-11-21
DOI
https://doi.org/10.1007/s41230-026-5291-2
Primary Topic
Additive Manufacturing Materials and Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Revealing Ti-6Al-4V process-microstructure-property relationships in high-speed annular laser directed energy deposition via in-situ monitoring

Kaiju Lu, LIANG Xiubing, Zelin Jiang, Kaixin Wang et al.
China Foundry
Additive Manufacturing Materials and Processes
article

Revealing Ti-6Al-4V process-microstructure-property relationships in high-speed annular laser directed energy deposition via in-situ monitoring

Kaiju Lu, LIANG Xiubing, Zelin Jiang, Kaixin Wang, Fa-Ming Li, Shu-yan Zhang, Zi-wei Zhu, Yong-xiong Chen
article en

Abstract

Although laser-directed energy deposition (L-DED) has been widely used owing to its high material utilization, short manufacturing cycle, and capability to fabricate large and complex components, conventional L-DED processes still face a trade-off between deposition rate and geometric accuracy, which restricts their application in areas requiring both high throughput and high precision. To address this trade-off, this work investigated off-axis powder feeding with a quasi-Gaussian laser beam and coaxial powder feeding with an annular laser beam during Ti-6Al-4V deposition at 12 and 36 mm·s −1 , aiming to clarify how the annular L-DED configuration affects process stability, deposition behavior, microstructural refinement, and mechanical properties under high-speed conditions. In-situ monitoring reveals that, under the high-speed deposition condition, the annular laser causes dominant energy absorption to shift from the substrate melt pool to the flying powder. Namely, as the scanning speed for the annular laser increases from 12 to 36 mm·s −1 , the average area and temperature of the melt pool decrease by 48.4% and 9.3%, respectively, and the spattering reduces significantly. This can be attributed to the redistribution of laser energy from the center toward the periphery by the annular beam, which improves the spatial overlap between the powder stream and laser energy, thereby forming a shallower and more stable melt pool. Thus, significant grain refinement is achieved in the deposition. In detail, microstructural analysis shows that the sample obtained using the annular laser at a high speed of 36 mm·s −1 exhibits the finest α-lath thickness (0.26±0.04 µm). Its mechanical properties follow the Hall-Petch relationship, with a tensile strength of 1,211.5 MPa, hardness of 394.8 HV 0.2 , and elongation of 7.0%. The high-speed annular L-DED process combines high efficiency, high strength, and excellent stability, providing a feasible route for additive manufacturing of advanced metallic components.

China Foundry
University of Electronic Science and Technology of China (CN)
Additive Manufacturing Materials and Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon