Interfacial strain accommodation in a castable nanostructured RAFM steel during 650 °C tensile deformation

Castable nanostructured alloys (CNAs) offer a scalable route to extend the high-temperature capability of reduced-activation ferritic/martensitic steels, yet their strain-accommodation behavior at 650 °C remains unclear. Under the present test condition, the CNA-derived RAFM steel exhibited a yield stress of 481.2 MPa, an ultimate tensile strength of 567.3 MPa and a total elongation of 26.18%. In-situ DIC, EBSD and TEM reveal a coupled response: MX/M23C6 interfaces and lath/sub-grain boundaries store dislocations, recovery-assisted rearrangement preserves matrix accommodation, and subsequent deformation is progressively confined to a necking zone. This interface-mediated hierarchy delays localization and produces the favorable 650 °C strength–ductility balance.

Authors

Publication Details

Journal
Figshare
Published
2026-11-21
DOI
https://doi.org/10.6084/m9.figshare.35081242
Primary Topic
Fusion materials and technologies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Interfacial strain accommodation in a castable nanostructured RAFM steel during 650 °C tensile deformation

Peter Kaehuei Liaw, Bingxin Cong, Jianzhong Jiang, Haoshang Liu et al.
Figshare
Fusion materials and technologies
article

Interfacial strain accommodation in a castable nanostructured RAFM steel during 650 °C tensile deformation

Peter Kaehuei Liaw, Bingxin Cong, Jianzhong Jiang, Haoshang Liu, Jiasheng Wang, Weipeng Cao, Jinru Luo, Tongde Shen, Yong Zhang
article en

Abstract

Castable nanostructured alloys (CNAs) offer a scalable route to extend the high-temperature capability of reduced-activation ferritic/martensitic steels, yet their strain-accommodation behavior at 650 °C remains unclear. Under the present test condition, the CNA-derived RAFM steel exhibited a yield stress of 481.2 MPa, an ultimate tensile strength of 567.3 MPa and a total elongation of 26.18%. In-situ DIC, EBSD and TEM reveal a coupled response: MX/M23C6 interfaces and lath/sub-grain boundaries store dislocations, recovery-assisted rearrangement preserves matrix accommodation, and subsequent deformation is progressively confined to a necking zone. This interface-mediated hierarchy delays localization and produces the favorable 650 °C strength–ductility balance.

Figshare
Fusion materials and technologies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines