Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments

Corrosion in oil and gas pipelines is strongly influenced by environmental chemistry and pipeline location, affecting reliability and safety. This study examines the corrosion behavior of API 5L X65 carbon steel under top (TLC) and bottom (BLC) conditions in sweet (CO 2 ) and sour (H 2 S/N 2 ) environments at 20 °C – 30 °C. Uniform corrosion rates (UCR) and pitting corrosion rates (PCR) were measured using weight loss (ASTM G1‐03) and surface profilometry (ASTM G46‐21), while scanning electron microscopy (SEM), energy dispersive x‐ray spectroscopy (EDX) and x‐ray diffraction (XRD) characterized surface morphology and corrosion products. In the sweet environment, top‐of‐the‐line corrosion and bottom‐of‐the‐line corrosion showed similar uniform corrosion rates (0.28 mm/y). Pitting corrosion was moderate, with pitting corrosion rates of 0.89 mm/y for top‐of‐the‐line corrosion and 0.67 mm/y for bottom‐of‐the‐line corrosion. Products were mainly thin Fe 3 C layers, with NaCl deposition only at the bottom. Under sour conditions, bottom‐of‐the‐line corrosion exhibited higher uniform corrosion rates (0.29 mm/y) than top‐of‐the‐line corrosion (0.22 mm/y), with more severe localized corrosion; pitting corrosion rate reached 1.94 mm/y at bottom‐of‐the‐line corrosion versus 0.43 mm/y at top‐of‐the‐line corrosion. Multilayered FeS scales formed in H 2 S environments, partially protecting the top, while bottom surfaces experienced combined sulfide and chloride attack, promoting localized pitting. These findings show that pipeline corrosion depends strongly on chemical environment and steel position, emphasizing the need for localized monitoring and targeted mitigation strategies to maintain pipeline integrity.

Authors

Institutions

Publication Details

Journal
Materialwissenschaft und Werkstofftechnik
Published
2026-11-20
DOI
https://doi.org/10.1002/mawe.70194
Primary Topic
Corrosion Behavior and Inhibition
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments

Najmiddin Yaakob, Norinsan Kamil Othman, Muhammad Taqiuddin, A. Md Noor
5 links
Materialwissenschaft und Werkstofftechnik
Corrosion Behavior and Inhibition
article

Top‐ and bottom‐of‐the‐line corrosion: Effects of 30 °C bottom liquid and 20 °C steel temperature in CO 2 and H 2 S/N 2 environments

Najmiddin Yaakob, Norinsan Kamil Othman, Muhammad Taqiuddin, A. Md Noor
article en

Abstract

Corrosion in oil and gas pipelines is strongly influenced by environmental chemistry and pipeline location, affecting reliability and safety. This study examines the corrosion behavior of API 5L X65 carbon steel under top (TLC) and bottom (BLC) conditions in sweet (CO 2 ) and sour (H 2 S/N 2 ) environments at 20 °C – 30 °C. Uniform corrosion rates (UCR) and pitting corrosion rates (PCR) were measured using weight loss (ASTM G1‐03) and surface profilometry (ASTM G46‐21), while scanning electron microscopy (SEM), energy dispersive x‐ray spectroscopy (EDX) and x‐ray diffraction (XRD) characterized surface morphology and corrosion products. In the sweet environment, top‐of‐the‐line corrosion and bottom‐of‐the‐line corrosion showed similar uniform corrosion rates (0.28 mm/y). Pitting corrosion was moderate, with pitting corrosion rates of 0.89 mm/y for top‐of‐the‐line corrosion and 0.67 mm/y for bottom‐of‐the‐line corrosion. Products were mainly thin Fe 3 C layers, with NaCl deposition only at the bottom. Under sour conditions, bottom‐of‐the‐line corrosion exhibited higher uniform corrosion rates (0.29 mm/y) than top‐of‐the‐line corrosion (0.22 mm/y), with more severe localized corrosion; pitting corrosion rate reached 1.94 mm/y at bottom‐of‐the‐line corrosion versus 0.43 mm/y at top‐of‐the‐line corrosion. Multilayered FeS scales formed in H 2 S environments, partially protecting the top, while bottom surfaces experienced combined sulfide and chloride attack, promoting localized pitting. These findings show that pipeline corrosion depends strongly on chemical environment and steel position, emphasizing the need for localized monitoring and targeted mitigation strategies to maintain pipeline integrity.

Materialwissenschaft und Werkstofftechnik
Universiti Teknologi MARA System (MY), Universiti Teknologi MARA (MY), National University of Malaysia (MY)
Universiti Teknologi MARA
Corrosion Behavior and Inhibition
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon