Effect of Cu addition on phase evolution, mechanical properties, corrosion behavior, and cytocompatibility of Ti–25Nb alloys fabricated by cold isostatic pressing

Titanium metal is widely used as an implant material due to its biocompatibility; however, further improvements are still required in terms of strength and corrosion resistance. This study evaluated the effect of Cu addition (0, 3, 6, and 9 wt.%) in Ti–25Nb alloys on microstructure, mechanical properties, corrosion resistance, and cytotoxic properties on MC-3T3-E1 cell lines. The alloy was fabricated using powder metallurgy via cold isostatic pressing at 30 MPa for 8 min. Then continued with a sintering process at 1300 °C for 4 h using a vacuum tube furnace with an inert environment using argon gas. X-ray diffraction analysis showed the formation of the Ti 2 Cu phase at high Cu content. The microstructure remains lamellar across all compositions, with progressive refinement of the lamellar structure observed as the Cu content increases, particularly at 6 and 9 wt.%. The crystallite size of the β-Ti phase increased from 26.1 nm for the Ti–25Nb alloy without copper addition to 43.6 nm for the alloy with 6 wt.% Cu; then the crystallite size decreased to 29.9 nm for the alloy with the addition of 9 wt.% Cu, indicating that excessive Ti 2 Cu precipitation could inhibit the growth of β crystals. It was shown that the hardness increased from 243.9 to 320.2 HV, and the density from 4.54 to 4.79 g/cm 3 . The alloy with 9 wt.% Cu had the lowest corrosion rate (0.000181 mm/year) and a corrosion current of 19 nA/cm 2 . The cytotoxicity results showed that the Ti–25Nb– x Cu alloys exhibited good biocompatibility with MC-3T3-E1 osteoblast cells, as cell viability values were above 90%. It is important to note that the Ti–25Nb alloy with 9 wt.% copper showed the best combination of microstructure, mechanical properties, and corrosion resistance, and is a potential candidate for medical implant applications.

Authors

Institutions

Publication Details

Journal
Powder Metallurgy
Published
2026-11-20
DOI
https://doi.org/10.1177/00325899261505087
Primary Topic
Titanium Alloys Microstructure and Properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effect of Cu addition on phase evolution, mechanical properties, corrosion behavior, and cytocompatibility of Ti–25Nb alloys fabricated by cold isostatic pressing

Dhyah Annur, Aprilia Erryani, Galih Senopati, A’liyatur Rosyidah et al.
2 links
Powder Metallurgy
Titanium Alloys Microstructure and Properties
article

Effect of Cu addition on phase evolution, mechanical properties, corrosion behavior, and cytocompatibility of Ti–25Nb alloys fabricated by cold isostatic pressing

Dhyah Annur, Aprilia Erryani, Galih Senopati, A’liyatur Rosyidah, Rahma Nisa Hakim, Albertus Deny Heri Setyawan, Adi Noer Syahid, Joko Triwardono, Edy Riyanto, Cahya Sutowo, Arif Tjahjono, Amelia Lestari, Yudi Nugraha Thaha, Ika Kartika, Fendy Rokhmanto
article en

Abstract

Titanium metal is widely used as an implant material due to its biocompatibility; however, further improvements are still required in terms of strength and corrosion resistance. This study evaluated the effect of Cu addition (0, 3, 6, and 9 wt.%) in Ti–25Nb alloys on microstructure, mechanical properties, corrosion resistance, and cytotoxic properties on MC-3T3-E1 cell lines. The alloy was fabricated using powder metallurgy via cold isostatic pressing at 30 MPa for 8 min. Then continued with a sintering process at 1300 °C for 4 h using a vacuum tube furnace with an inert environment using argon gas. X-ray diffraction analysis showed the formation of the Ti 2 Cu phase at high Cu content. The microstructure remains lamellar across all compositions, with progressive refinement of the lamellar structure observed as the Cu content increases, particularly at 6 and 9 wt.%. The crystallite size of the β-Ti phase increased from 26.1 nm for the Ti–25Nb alloy without copper addition to 43.6 nm for the alloy with 6 wt.% Cu; then the crystallite size decreased to 29.9 nm for the alloy with the addition of 9 wt.% Cu, indicating that excessive Ti 2 Cu precipitation could inhibit the growth of β crystals. It was shown that the hardness increased from 243.9 to 320.2 HV, and the density from 4.54 to 4.79 g/cm 3 . The alloy with 9 wt.% Cu had the lowest corrosion rate (0.000181 mm/year) and a corrosion current of 19 nA/cm 2 . The cytotoxicity results showed that the Ti–25Nb– x Cu alloys exhibited good biocompatibility with MC-3T3-E1 osteoblast cells, as cell viability values were above 90%. It is important to note that the Ti–25Nb alloy with 9 wt.% copper showed the best combination of microstructure, mechanical properties, and corrosion resistance, and is a potential candidate for medical implant applications.

Powder Metallurgy
Syarif Hidayatullah State Islamic University Jakarta (ID), Universitas Gadjah Mada (ID), National Research and Innovation Agency (ID)
Good health and well-being
Titanium Alloys Microstructure and Properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon