Assessment of gaseous hydrogen embrittlement in welds using sub-size tensile specimens

This study investigates hydrogen embrittlement in an X60 steel girth weld using sub-size tensile specimens extracted from the base metal (BM), weld metal (WM), and cross-weld (CW). Tests were performed in air and under 200 bar H 2 using an optical extensometry-based setup. Results show that hydrogen has no significant effect on yield or ultimate tensile strength, but strongly reduces ductility, with reduction of area decreasing from 78.9% to 29.4% in the BM and from 66.9% to 33.0% in the WM. Fractography and tomography analysis reveal a transition from ductile central void coalescence in air to early surface-initiated quasi-brittle cracking under hydrogen, with inclined crack propagation at ∼ 50° relative to the loading axis. EBSD analysis locates cracks near the BM–HAZ (heat-affected zone) interface, where the softer HAZ and mechanical heterogeneity may contribute to damage localization. The methodology involving sub-size specimens provides a framework for interpreting hydrogen damage in welded structures.

Authors

Institutions

Publication Details

Journal
International Journal of Hydrogen Energy
Published
2026-11-20
DOI
https://doi.org/10.1016/j.ijhydene.2026.158617
Primary Topic
Hydrogen embrittlement and corrosion behaviors in metals
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Assessment of gaseous hydrogen embrittlement in welds using sub-size tensile specimens

Livia Cupertino-Malheiros, Yazid Madi, Sangchu Quan, Luciano Meirelles Santana et al.
International Journal of Hydrogen Energy
Hydrogen embrittlement and corrosion behaviors in metals
article

Assessment of gaseous hydrogen embrittlement in welds using sub-size tensile specimens

Livia Cupertino-Malheiros, Yazid Madi, Sangchu Quan, Luciano Meirelles Santana, A. King, V. Okumko
article en

Abstract

This study investigates hydrogen embrittlement in an X60 steel girth weld using sub-size tensile specimens extracted from the base metal (BM), weld metal (WM), and cross-weld (CW). Tests were performed in air and under 200 bar H 2 using an optical extensometry-based setup. Results show that hydrogen has no significant effect on yield or ultimate tensile strength, but strongly reduces ductility, with reduction of area decreasing from 78.9% to 29.4% in the BM and from 66.9% to 33.0% in the WM. Fractography and tomography analysis reveal a transition from ductile central void coalescence in air to early surface-initiated quasi-brittle cracking under hydrogen, with inclined crack propagation at ∼ 50° relative to the loading axis. EBSD analysis locates cracks near the BM–HAZ (heat-affected zone) interface, where the softer HAZ and mechanical heterogeneity may contribute to damage localization. The methodology involving sub-size specimens provides a framework for interpreting hydrogen damage in welded structures.

International Journal of Hydrogen EnergyVol. 294
Centre National de la Recherche Scientifique (FR), Synchrotron soleil (FR), Centre des Matériaux (FR), Imperial College London (GB)
Agence Nationale de la Recherche, Engineering and Physical Sciences Research Council
Hydrogen embrittlement and corrosion behaviors in metals
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
Assessment of gaseous hydrogen embrittlement in welds using sub-size tensile specimens — Livia Cupertino-Malheiros, Yazid Madi, et al. · International Journal of Hydrogen Energy (2026) | TGRS Research Map | TGRS