Phase Evolution and Thermodynamic Feasibility of γ - Fe2O3 Formation from Iron Ore Concentrate via Spark Plasma Sintering

The evolution of iron oxide phases during Spark Plasma Sintering (SPS) was examined using hematite-rich concentrate obtained from the Hudagt deposit in Mongolia. The initial powder contained predominantly a - Fe 2 O 3 with minor Fe 3 O 4 , and no detectable γ - Fe 2 O 3 . Sintering was performed under vacuum (~5 Pa) at temperatures between 500 and 700 °C with holding times ranging from 5 to 30 min. At 500 °C, a substantial fraction of γ - Fe 2 O 3 (~70.96%) developed, accompanied by residual magnetite. Increasing temperature or prolonging the dwell time progressively favored reappearance of α - Fe 2 O 3 . These observations suggest that, within a limited thermal window, oxidation of inside the spinel framework can proceed without triggering full reconstructive transformation to the corundum structure. Rapid heating and restricted diffusion during SPS appear to temporarily preserve the defect-spinel configuration. The results highlight the importance of kinetic constraint in stabilizing γ - Fe 2 O 3 directly from hematite-dominant natural ore.

Authors

Institutions

Publication Details

Journal
Key engineering materials
Published
2026-11-24
DOI
https://doi.org/10.4028/p-zre8hl
Primary Topic
Iron oxide chemistry and applications
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Phase Evolution and Thermodynamic Feasibility of γ - Fe2O3 Formation from Iron Ore Concentrate via Spark Plasma Sintering

D. Ganbat, Masao Tokita, Mangal Delgermaa, Batsukh Tuvdendorj
1 links
Key engineering materials
Iron oxide chemistry and applications
article

Phase Evolution and Thermodynamic Feasibility of γ - Fe2O3 Formation from Iron Ore Concentrate via Spark Plasma Sintering

D. Ganbat, Masao Tokita, Mangal Delgermaa, Batsukh Tuvdendorj
article en

Abstract

The evolution of iron oxide phases during Spark Plasma Sintering (SPS) was examined using hematite-rich concentrate obtained from the Hudagt deposit in Mongolia. The initial powder contained predominantly a - Fe 2 O 3 with minor Fe 3 O 4 , and no detectable γ - Fe 2 O 3 . Sintering was performed under vacuum (~5 Pa) at temperatures between 500 and 700 °C with holding times ranging from 5 to 30 min. At 500 °C, a substantial fraction of γ - Fe 2 O 3 (~70.96%) developed, accompanied by residual magnetite. Increasing temperature or prolonging the dwell time progressively favored reappearance of α - Fe 2 O 3 . These observations suggest that, within a limited thermal window, oxidation of inside the spinel framework can proceed without triggering full reconstructive transformation to the corundum structure. Rapid heating and restricted diffusion during SPS appear to temporarily preserve the defect-spinel configuration. The results highlight the importance of kinetic constraint in stabilizing γ - Fe 2 O 3 directly from hematite-dominant natural ore.

Key engineering materialsVol. 1065
Mongolian University of Science and Technology (MN)
Iron oxide chemistry and applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon