Coating Deposition of Aldehyde‐Ketone Resin Onto Carboxylated Carbon Fibers: Surface Chemistry, Micro‐Morphology, Wettability, Monofilament Mechanical and Interfacial Shear Properties

In this work, domestic PAN‐based T700 carbon fibers (CF; “T” denotes tensile‐strength grade, nominal tensile strength ≥ 4900 MPa, monofilament diameter ~7 μm) were activated by nitric acid carboxylation to generate abundant polar oxygen‐containing functional groups on fiber surfaces. AK (aldehyde‐ketone) resin coatings with two concentrations (50 and 100 wt%) were fabricated through a facile solution impregnation route. A set of characterization techniques, including scanning electron microscopy (SEM), X‐ray photoelectron spectroscopy (XPS), Raman spectroscopy, contact angle testing, atomic force microscopy (AFM), monofilament tensile measurements and microdroplet debonding tests, were carried out to reveal the dependence of surface morphology, chemical constitution, wettability, single‐fiber mechanical response and interfacial shear strength (IFSS) of modified carbon fibers on resin concentration. Nitric acid etching raises the surface O/C atomic ratio from 14.49% to 26.79% and introduces minor surface micro‐pits on fiber surfaces. The AK resin forms continuous coatings via physical encapsulation and plausible intermolecular hydrogen‐bonding interactions with fiber‐surface carboxyl groups. The rising resin concentration modulates surface roughness and water affinity. The 100 wt% AK‐coated carbon fiber achieves the optimal overall performance, with its water contact angle reduced to 82.032° and greatly improved monofilament tensile load. Compared with oxidized OCF with an IFSS of 10.978 MPa, the IFSS values of OCF‐50 wt% AK and OCF‐100 wt% AK reach 13.030 and 13.540 MPa, respectively. This low‐cost, controllable surface modification approach avoids expensive nanofillers and harsh treatment conditions, which offers a reliable scheme for tuning the surface physicochemical characteristics of CF.

Authors

Institutions

Publication Details

Journal
Polymer Composites
Published
2026-11-18
DOI
https://doi.org/10.1002/pc.71844
Primary Topic
Fiber-reinforced polymer composites
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Coating Deposition of Aldehyde‐Ketone Resin Onto Carboxylated Carbon Fibers: Surface Chemistry, Micro‐Morphology, Wettability, Monofilament Mechanical and Interfacial Shear Properties

Li Yu, Zhengwei Yang
Polymer Composites
Fiber-reinforced polymer composites
article

Coating Deposition of Aldehyde‐Ketone Resin Onto Carboxylated Carbon Fibers: Surface Chemistry, Micro‐Morphology, Wettability, Monofilament Mechanical and Interfacial Shear Properties

Li Yu, Zhengwei Yang
article en

Abstract

In this work, domestic PAN‐based T700 carbon fibers (CF; “T” denotes tensile‐strength grade, nominal tensile strength ≥ 4900 MPa, monofilament diameter ~7 μm) were activated by nitric acid carboxylation to generate abundant polar oxygen‐containing functional groups on fiber surfaces. AK (aldehyde‐ketone) resin coatings with two concentrations (50 and 100 wt%) were fabricated through a facile solution impregnation route. A set of characterization techniques, including scanning electron microscopy (SEM), X‐ray photoelectron spectroscopy (XPS), Raman spectroscopy, contact angle testing, atomic force microscopy (AFM), monofilament tensile measurements and microdroplet debonding tests, were carried out to reveal the dependence of surface morphology, chemical constitution, wettability, single‐fiber mechanical response and interfacial shear strength (IFSS) of modified carbon fibers on resin concentration. Nitric acid etching raises the surface O/C atomic ratio from 14.49% to 26.79% and introduces minor surface micro‐pits on fiber surfaces. The AK resin forms continuous coatings via physical encapsulation and plausible intermolecular hydrogen‐bonding interactions with fiber‐surface carboxyl groups. The rising resin concentration modulates surface roughness and water affinity. The 100 wt% AK‐coated carbon fiber achieves the optimal overall performance, with its water contact angle reduced to 82.032° and greatly improved monofilament tensile load. Compared with oxidized OCF with an IFSS of 10.978 MPa, the IFSS values of OCF‐50 wt% AK and OCF‐100 wt% AK reach 13.030 and 13.540 MPa, respectively. This low‐cost, controllable surface modification approach avoids expensive nanofillers and harsh treatment conditions, which offers a reliable scheme for tuning the surface physicochemical characteristics of CF.

Polymer Composites
PLA Rocket Force University of Engineering (CN)
Fiber-reinforced polymer composites
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon