The effect of wall thickness and MWCNT concentration on the piezoresistive properties of Gyroid lattice structures produced from MWCNT-reinforced PLA and ABS filaments

In this study, the mechanical, thermal, electrical, and piezoresistive performances of Gyroid lattice structures produced from multi-walled carbon nanotube (MWCNT)-reinforced PLA and ABS filaments using the fused filament fabrication (FFF) method were comparatively investigated. MWCNT was added to the PLA and ABS matrices at ratios of 3% and 5%, and Gyroid lattice-structured specimens with dimensions of 16 × 16 × 24 mm and wall thicknesses of 0.60, 0.80, and 1.00 mm were produced. The structural and thermal properties of the composites were evaluated through Fourier Transform Infrared Spectroscopy (FTIR), thermogravimetric analysis (TGA), differential thermal analysis (DTA), and differential scanning calorimetry (DSC) analyses, while their mechanical behavior was determined by uniaxial compression tests. Electrical conductivity and gauge factor variations were measured under compressive deformation, and their piezoresistive performance was analyzed. The results showed that increasing the wall thickness enhanced the compressive strength and structural stability of the Gyroid structures throughout deformation. The composites containing 5% MWCNT exhibited higher initial electrical conductivity; while the specimens produced using PLA reached higher conductivity values compared to those produced using ABS. In contrast, the highest low-strain piezoresistive sensitivity was obtained with the combination of 3% MWCNT-PLA and a 1.00 mm wall thickness. The 5% MWCNT-ABS specimens exhibited a more regular and stable gauge factor behavior over a wide strain range. The findings demonstrate that MWCNT-reinforced Gyroid lattice structures produced by FFF can be used as tunable and multifunctional piezoresistive structures that combine mechanical load-bearing capacity with deformation-sensing functionality.

Authors

Institutions

Publication Details

Journal
Journal of Thermoplastic Composite Materials
Published
2026-11-19
DOI
https://doi.org/10.1177/08927057261510473
Primary Topic
Cellular and Composite Structures
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

The effect of wall thickness and MWCNT concentration on the piezoresistive properties of Gyroid lattice structures produced from MWCNT-reinforced PLA and ABS filaments

Özgün Ceren Akbay, Süleyman Köytepe, Mustafa Ercan Gündüz, Erkan Bahçe
Journal of Thermoplastic Composite Materials
Cellular and Composite Structures
article

The effect of wall thickness and MWCNT concentration on the piezoresistive properties of Gyroid lattice structures produced from MWCNT-reinforced PLA and ABS filaments

Özgün Ceren Akbay, Süleyman Köytepe, Mustafa Ercan Gündüz, Erkan Bahçe
article en

Abstract

In this study, the mechanical, thermal, electrical, and piezoresistive performances of Gyroid lattice structures produced from multi-walled carbon nanotube (MWCNT)-reinforced PLA and ABS filaments using the fused filament fabrication (FFF) method were comparatively investigated. MWCNT was added to the PLA and ABS matrices at ratios of 3% and 5%, and Gyroid lattice-structured specimens with dimensions of 16 × 16 × 24 mm and wall thicknesses of 0.60, 0.80, and 1.00 mm were produced. The structural and thermal properties of the composites were evaluated through Fourier Transform Infrared Spectroscopy (FTIR), thermogravimetric analysis (TGA), differential thermal analysis (DTA), and differential scanning calorimetry (DSC) analyses, while their mechanical behavior was determined by uniaxial compression tests. Electrical conductivity and gauge factor variations were measured under compressive deformation, and their piezoresistive performance was analyzed. The results showed that increasing the wall thickness enhanced the compressive strength and structural stability of the Gyroid structures throughout deformation. The composites containing 5% MWCNT exhibited higher initial electrical conductivity; while the specimens produced using PLA reached higher conductivity values compared to those produced using ABS. In contrast, the highest low-strain piezoresistive sensitivity was obtained with the combination of 3% MWCNT-PLA and a 1.00 mm wall thickness. The 5% MWCNT-ABS specimens exhibited a more regular and stable gauge factor behavior over a wide strain range. The findings demonstrate that MWCNT-reinforced Gyroid lattice structures produced by FFF can be used as tunable and multifunctional piezoresistive structures that combine mechanical load-bearing capacity with deformation-sensing functionality.

Journal of Thermoplastic Composite Materials
Inonu University (TR)
Cellular and Composite Structures
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon