Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments

ABSTRACT Fiber‐reinforced polymer (FRP) composites may undergo mechanical degradation in aggressive chemical environments, while concentration‐dependent differences between acidic and alkaline exposure remain insufficiently characterized for the same GFRP bar system. In this study, pultruded vinyl‐ester GFRP bars were exposed at room temperature to H 2 SO 4 and NaOH solutions with concentrations ranging from 0.5 to 3.0 mol/L for 30 and 60 days. Density, tensile strength, and shear strength were evaluated, while SEM, qualitative EDS, and FTIR were used to characterize local material changes. Under H 2 SO 4 exposure, tensile‐strength retention remained at or above 97.0%, whereas shear‐strength retention decreased to 92.6% after 60 days in 3.0 mol/L solution. Localized fiber‐surface roughening and gaps near some fiber/resin boundaries were observed. Under NaOH exposure, tensile‐strength retention decreased to 90.0% under the same concentration and duration, while shear‐strength retention remained at 98.4%. More evident surface‐resin loss and fiber exposure were observed, and the FTIR results were consistent with alteration of the vinyl‐ester matrix. Thus, the same GFRP bar system exhibited a greater relative reduction in shear strength under H 2 SO 4 exposure but a greater relative reduction in tensile strength under NaOH exposure. An empirical semi‐logarithmic relationship was used to compare the apparent degradation rates only within the measured 0–60‐day interval. These results highlight the value of jointly assessing tensile and shear retention when characterizing the short‐term chemical durability of GFRP bars.

Authors

Institutions

Publication Details

Journal
Polymer Composites
Published
2026-11-17
DOI
https://doi.org/10.1002/pc.71876
Primary Topic
Structural Behavior of Reinforced Concrete
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments

Benxiang Tan, Tong Liu, Zhenghua Mao, Yunxia Wang et al.
Polymer Composites
Structural Behavior of Reinforced Concrete
article

Microstructural Evolution and Differential Mechanical Degradation Mechanisms of GFRP Bars in Acidic and Alkaline Environments

Benxiang Tan, Tong Liu, Zhenghua Mao, Yunxia Wang, Chao Peng, Xinghai Li
article en

Abstract

ABSTRACT Fiber‐reinforced polymer (FRP) composites may undergo mechanical degradation in aggressive chemical environments, while concentration‐dependent differences between acidic and alkaline exposure remain insufficiently characterized for the same GFRP bar system. In this study, pultruded vinyl‐ester GFRP bars were exposed at room temperature to H 2 SO 4 and NaOH solutions with concentrations ranging from 0.5 to 3.0 mol/L for 30 and 60 days. Density, tensile strength, and shear strength were evaluated, while SEM, qualitative EDS, and FTIR were used to characterize local material changes. Under H 2 SO 4 exposure, tensile‐strength retention remained at or above 97.0%, whereas shear‐strength retention decreased to 92.6% after 60 days in 3.0 mol/L solution. Localized fiber‐surface roughening and gaps near some fiber/resin boundaries were observed. Under NaOH exposure, tensile‐strength retention decreased to 90.0% under the same concentration and duration, while shear‐strength retention remained at 98.4%. More evident surface‐resin loss and fiber exposure were observed, and the FTIR results were consistent with alteration of the vinyl‐ester matrix. Thus, the same GFRP bar system exhibited a greater relative reduction in shear strength under H 2 SO 4 exposure but a greater relative reduction in tensile strength under NaOH exposure. An empirical semi‐logarithmic relationship was used to compare the apparent degradation rates only within the measured 0–60‐day interval. These results highlight the value of jointly assessing tensile and shear retention when characterizing the short‐term chemical durability of GFRP bars.

Polymer Composites
Guizhou University (CN), Liupanshui Normal University (CN)
Structural Behavior of Reinforced Concrete
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon