Influence of cooling route on microstructure, mechanical performance, and erosion resistance of ASTM A537 pressure vessel steel

This study investigates the effects of cooling severity on the microstructure, mechanical properties, and solid particle erosion behavior of ASTM A537 pressure-vessel steel. Specimens were austenitized at 900 °C and subjected to air cooling, salt-bath cooling at 300 °C, oil quenching, and water quenching, followed by tempering of the water-quenched condition. The microstructure evolved from ferrite–pearlite (FP) in the air-cooled condition to predominantly bainitic ferrite (BF) with substantial retained austenite (RA) in the salt-bath cooled condition, finer BF with lower RA and a possible minor martensitic contribution in the oil-cooled condition, and predominantly martensitic (M) structure after water quenching. Increasing cooling severity (in the order A537A < A537S < A537O < A537W) increased yield strength, compressive strength and hardness, whereas UTS gains were limited to the water-quenched condition and ductility generally decreased. The water-quenched condition exhibited the highest yield strength (530 MPa), ultimate tensile strength (630 MPa), compressive yield strength (610 MPa), and hardness (431 HV), while the air-cooled condition showed the highest elongation (38%). Notably, the water-quenched condition retained a relatively high elongation of approximately 28% despite its predominantly martensitic structure. Fractographic analysis revealed predominantly ductile dimple rupture in the salt-bath and oil-cooled conditions, whereas the water-quenched condition exhibited a mixed, lath-controlled tearing morphology with localized microvoid coalescence. Solid particle erosion tests at a 45° impact angle, performed on the FP (air-cooled) and martensitic (water-quenched) conditions, showed a strong relationship between hardness and erosion resistance, with the water-quenched condition exhibiting approximately half the mass loss of the FP condition after 15 min. These findings establish a structure–property–erosion relationship for A537 steel and provide a basis for selecting heat-treatment routes, pending further evaluation of toughness and service performance for pressure-vessel applications.

Authors

Institutions

Publication Details

Journal
Next Materials
Published
2026-11-18
DOI
https://doi.org/10.1016/j.nxmate.2026.104086
Primary Topic
Microstructure and Mechanical Properties of Steels
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Influence of cooling route on microstructure, mechanical performance, and erosion resistance of ASTM A537 pressure vessel steel

Mohsen Reihanian, Khalil Ranjbar, M.N. Roghanian
Next Materials
Microstructure and Mechanical Properties of Steels
article

Influence of cooling route on microstructure, mechanical performance, and erosion resistance of ASTM A537 pressure vessel steel

Mohsen Reihanian, Khalil Ranjbar, M.N. Roghanian
article en

Abstract

This study investigates the effects of cooling severity on the microstructure, mechanical properties, and solid particle erosion behavior of ASTM A537 pressure-vessel steel. Specimens were austenitized at 900 °C and subjected to air cooling, salt-bath cooling at 300 °C, oil quenching, and water quenching, followed by tempering of the water-quenched condition. The microstructure evolved from ferrite–pearlite (FP) in the air-cooled condition to predominantly bainitic ferrite (BF) with substantial retained austenite (RA) in the salt-bath cooled condition, finer BF with lower RA and a possible minor martensitic contribution in the oil-cooled condition, and predominantly martensitic (M) structure after water quenching. Increasing cooling severity (in the order A537A < A537S < A537O < A537W) increased yield strength, compressive strength and hardness, whereas UTS gains were limited to the water-quenched condition and ductility generally decreased. The water-quenched condition exhibited the highest yield strength (530 MPa), ultimate tensile strength (630 MPa), compressive yield strength (610 MPa), and hardness (431 HV), while the air-cooled condition showed the highest elongation (38%). Notably, the water-quenched condition retained a relatively high elongation of approximately 28% despite its predominantly martensitic structure. Fractographic analysis revealed predominantly ductile dimple rupture in the salt-bath and oil-cooled conditions, whereas the water-quenched condition exhibited a mixed, lath-controlled tearing morphology with localized microvoid coalescence. Solid particle erosion tests at a 45° impact angle, performed on the FP (air-cooled) and martensitic (water-quenched) conditions, showed a strong relationship between hardness and erosion resistance, with the water-quenched condition exhibiting approximately half the mass loss of the FP condition after 15 min. These findings establish a structure–property–erosion relationship for A537 steel and provide a basis for selecting heat-treatment routes, pending further evaluation of toughness and service performance for pressure-vessel applications.

Next MaterialsVol. 14
Shahid Chamran University of Ahvaz (IR)
Shahid Chamran University of Ahvaz
Microstructure and Mechanical Properties of Steels
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon