From Powder to Cementitious Matrix: Correlating Physico-Chemical Properties of Photocatalysts with NOx Abatement and Self-Cleaning Performance of Cement Mortars

The photocatalytic performance of TiO2 powders is commonly associated with specific surface area, crystallite size, and phase composition; however, the extent to which these characteristics remain relevant after incorporation into cementitious materials is not well established. This study investigated nine commercial TiO2 photocatalysts spanning BET surface areas of 53.8–360.6 m2/g. The powders were physicochemically characterized and evaluated for NOx abatement, after which seven representative photocatalysts were incorporated into cement mortars at dosages of 4–18 kg/m3 and tested for NOx removal and self-cleaning performance. At the powder scale, NO removal generally increased with BET surface area, although the improvement diminished above approximately 200–240 m2/g. Incorporation into mortar fundamentally altered this relationship. P25, despite having the lowest BET surface area and powder-scale NO removal, exhibited the highest mortar-scale activity, exceeding 220 μg/(m2·h), whereas high-BET photocatalysts generally remained below 80 μg/(m2·h). DLS and SEM/EDS analyses indicated that composite-scale performance was more closely associated with photocatalyst accessibility after hydration than with nominal powder surface area or agglomerate size alone. Two complementary indicators were therefore introduced: the Photocatalytic Utility Index (PUI), quantifying overall powder-to-composite performance transfer, and the Dose–Response Index (DRI), quantifying response to increasing photocatalyst content. Low-BET photocatalysts exhibited substantially higher PUI and DRI values than high-BET materials.

Authors

Institutions

Publication Details

Journal
Catalysts
Published
2026-11-18
DOI
https://doi.org/10.3390/catal16111029
Primary Topic
TiO2 Photocatalysis and Solar Cells
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

From Powder to Cementitious Matrix: Correlating Physico-Chemical Properties of Photocatalysts with NOx Abatement and Self-Cleaning Performance of Cement Mortars

Karol Chilmon, Maciej Kalinowski, Beata Jaworska, Filip Chyliński et al.
Catalysts
TiO2 Photocatalysis and Solar Cells
article

From Powder to Cementitious Matrix: Correlating Physico-Chemical Properties of Photocatalysts with NOx Abatement and Self-Cleaning Performance of Cement Mortars

Karol Chilmon, Maciej Kalinowski, Beata Jaworska, Filip Chyliński, Wioletta Jackiewicz-Rek
article en

Abstract

The photocatalytic performance of TiO2 powders is commonly associated with specific surface area, crystallite size, and phase composition; however, the extent to which these characteristics remain relevant after incorporation into cementitious materials is not well established. This study investigated nine commercial TiO2 photocatalysts spanning BET surface areas of 53.8–360.6 m2/g. The powders were physicochemically characterized and evaluated for NOx abatement, after which seven representative photocatalysts were incorporated into cement mortars at dosages of 4–18 kg/m3 and tested for NOx removal and self-cleaning performance. At the powder scale, NO removal generally increased with BET surface area, although the improvement diminished above approximately 200–240 m2/g. Incorporation into mortar fundamentally altered this relationship. P25, despite having the lowest BET surface area and powder-scale NO removal, exhibited the highest mortar-scale activity, exceeding 220 μg/(m2·h), whereas high-BET photocatalysts generally remained below 80 μg/(m2·h). DLS and SEM/EDS analyses indicated that composite-scale performance was more closely associated with photocatalyst accessibility after hydration than with nominal powder surface area or agglomerate size alone. Two complementary indicators were therefore introduced: the Photocatalytic Utility Index (PUI), quantifying overall powder-to-composite performance transfer, and the Dose–Response Index (DRI), quantifying response to increasing photocatalyst content. Low-BET photocatalysts exhibited substantially higher PUI and DRI values than high-BET materials.

CatalystsVol. 16(11)
Warsaw University of Technology (PL), Instytut Techniki Budowlanej (PL)
Politechnika Warszawska
TiO2 Photocatalysis and Solar Cells
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon