Environmental Effects on Strength and Drying Shrinkage of Cement-Stabilized Aeolian Sand–Aggregate Bases
This study compared strength retention and subsequent drying shrinkage of cement-stabilized aeolian sand–aggregate bases under four environmental exposures. Four mixtures combined total binder contents of 6% and 7% with aeolian sand contents of 32% and 41%. After 28 d of standard curing, separate specimen groups underwent low-temperature exposure, hot–dry exposure, thermal cycling, or sulfate freeze–thaw cycling. Strength was evaluated after 7 and 28 d of additional exposure; independent groups underwent 7 d of pre-exposure followed by 15 d of drying measurements. Relative to age-matched controls, hot–dry strength was numerically 4.1% higher at 7 d but 24.7% lower at 28 d, averaged across mixtures. Day-15 shrinkage after hot–dry pre-exposure was 20.3% higher. Sulfate freeze–thaw cycling produced the lowest average strength retention at 7 d (79.3%), whereas thermal cycling produced the lowest retention at 28 d (65.7%). Higher binder content corresponded to greater 28 d strength retention and greater drying shrinkage. Lower aeolian sand content corresponded to greater residual strength and lower shrinkage. These descriptive comparisons indicate that mixture assessment should consider exposure duration, absolute performance, and relative changes.
Authors
- Xiaoping Ji (ORCID: https://orcid.org/0000-0003-3832-6877)
- Jianxiang Wang (ORCID: https://orcid.org/0009-0009-6021-7555)
- 拂晓
- Wenjie Shang (ORCID: https://orcid.org/0009-0008-7578-8759)
- Xuekui Wang
- Yuxin Luo
Institutions
- Chang'an University (CN)
- China Academy of Transportation Sciences (CN)
Publication Details
- Journal
- Materials
- Published
- 2026-11-18
- DOI
- https://doi.org/10.3390/ma19224875
- Primary Topic
- Geotechnical and construction materials studies
- Type
- article
- Field-Weighted Citation Impact
- 0.00