Effects of Humic and Fulvic Acid Composition on Strength and Immersion Resistance of Solid Waste-Based Stabilised Soil
For use as engineered fill, stabilised soil must develop adequate strength and retain it during water exposure. How fulvic acid (FAc) and humic acid (HAc) jointly affect these properties remains unclear. Twenty-five mixtures were prepared at varying acid dosages and a fixed carbide slag–ground granulated blast-furnace slag–fly ash (CGF) dosage. After 7 d of initial curing, unconfined compressive strength (UCS) was measured during continued chamber curing or immersion for up to 90 d. At 1.2% total acid, increasing FAc from 1:3 to 3:1 reduced 97 d UCS from 6.87 to 3.91 MPa. The corresponding UCS retention after 28 d of immersion decreased from 45.09% to 3.36% relative to age-matched chamber-cured controls. The chamber-curing model combined age-dependent strength development with an acid-dependent strength-retention factor, KFH (R2 = 0.92). The composition- and time-dependent immersion coefficient KW linked immersed UCS to age-matched chamber-cured strength (R2 = 0.94). Microscopy and tomography showed less continuous cementation and greater pore interconnection in the FAc-rich mixture. Calcium binding by FAc and HAc may alter calcium availability for cementitious reactions and affect the formation of interparticle bonds. During immersion, the migration of dissolved constituents may further weaken these bonds. Acid composition should therefore inform assessments of CGF-stabilised fill exposed to water.
Authors
- Kai Yao (ORCID: https://orcid.org/0000-0001-8846-5184)
- Qigang Chan
- Changjiang Dong
- Xincheng Xu
Institutions
- Shandong University (CN)
Publication Details
- Journal
- Materials
- Published
- 2026-11-18
- DOI
- https://doi.org/10.3390/ma19224883
- Primary Topic
- Geotechnical Engineering and Soil Stabilization
- Type
- article
- Field-Weighted Citation Impact
- 0.00