Evaluation of topography, color stability, and fracture resistance of prefabricated primary crowns with different material compositions: an in vitro study

Background Full coverage of primary teeth with stainless steel crowns (SSC) has shown limited esthetic acceptance. Few studies have investigated hybrid polymer-based crowns (HPC) under critical loading in comparison with SSC and prefabricated zirconia crowns (ZRC) in vitro. Aim This in vitro study compared wear, wear of antagonist teeth, vertical marginal gap, fracture resistance, and color stability of HPCs with those of SSCs and ZRCs. Methods Fifteen 3D-printed identical dies were fabricated to receive prefabricated crowns, which were divided into 3 groups: (1) stainless steel (SSCs), (2) zirconia (ZRCs), and (3) hybrid polymer-based (HPCs). Vertical marginal gap was assessed by measuring the vertical distance between the crown and die margins before and after thermomechanical ageing to simulate 1 year. Crowns were optically scanned to analyse the average surface roughness. Wear assessment via Geomagic software was performed for crowns and antagonist teeth. Color change was evaluated via digital imaging method. Fracture resistance was assessed by applying a load until fracture, then failure mode was evaluated. Data were assessed with Kolmogorov–Smirnov and Shapiro–Wilk tests. Intergroup comparisons were performed using one-way ANOVA and Tukey’s post hoc test; intragroup comparisons used paired t-tests, and categorical data analysed with chi-square test. Results Statistically significant differences were found in the vertical marginal gap, where HPCs had the highest value, followed by ZRCs and SSCs ( P < 0.001); however, these values were all within clinically acceptable range. There was no statistically significant difference in surface roughness ( P > 0.016). SSCs presented the greatest amount of wear, followed by HPCs and ZRCs ( P < 0.001). Hybrid polymer-based crowns showed the greatest color change, followed by ZRCs ( P < 0.001). HPCs showed the greatest color change ( P < 0.001). SSCs had the highest fracture resistance (1713.00 ± 181.84 N), whereas HPCs (980.72 ± 132.41 N) and ZRCs (1039.63 ± 209.21 N) did not differ significantly. HPCs and SSCs exhibited surface deformation and microperforations, whereas ZRCs exhibited fracture. Conclusions HPCs, ZRCs, and SSCs had vertical marginal gap values within the clinically acceptable range, and no significant differences were found in surface roughness between groups. HPCs showed lower crown wear than SSCs and lower antagonist wear than ZRCs and SSCs. HPCs exhibited greater color change than ZRCs, while their fracture resistance was not significantly different from that of ZRCs.

Authors

Institutions

Publication Details

Journal
BMC Oral Health
Published
2026-11-18
DOI
https://doi.org/10.1186/s12903-026-10175-y
Primary Topic
Dental materials and restorations
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Evaluation of topography, color stability, and fracture resistance of prefabricated primary crowns with different material compositions: an in vitro study

Osama Ibrahim El Shahawy, Maii Mohamed, Aiah A. El‐Rashidy, Omar Osama Shaalan et al.
7 links
BMC Oral Health
Dental materials and restorations
article

Evaluation of topography, color stability, and fracture resistance of prefabricated primary crowns with different material compositions: an in vitro study

Osama Ibrahim El Shahawy, Maii Mohamed, Aiah A. El‐Rashidy, Omar Osama Shaalan, Mohamed Amr ElKhashab
article en

Abstract

Background Full coverage of primary teeth with stainless steel crowns (SSC) has shown limited esthetic acceptance. Few studies have investigated hybrid polymer-based crowns (HPC) under critical loading in comparison with SSC and prefabricated zirconia crowns (ZRC) in vitro. Aim This in vitro study compared wear, wear of antagonist teeth, vertical marginal gap, fracture resistance, and color stability of HPCs with those of SSCs and ZRCs. Methods Fifteen 3D-printed identical dies were fabricated to receive prefabricated crowns, which were divided into 3 groups: (1) stainless steel (SSCs), (2) zirconia (ZRCs), and (3) hybrid polymer-based (HPCs). Vertical marginal gap was assessed by measuring the vertical distance between the crown and die margins before and after thermomechanical ageing to simulate 1 year. Crowns were optically scanned to analyse the average surface roughness. Wear assessment via Geomagic software was performed for crowns and antagonist teeth. Color change was evaluated via digital imaging method. Fracture resistance was assessed by applying a load until fracture, then failure mode was evaluated. Data were assessed with Kolmogorov–Smirnov and Shapiro–Wilk tests. Intergroup comparisons were performed using one-way ANOVA and Tukey’s post hoc test; intragroup comparisons used paired t-tests, and categorical data analysed with chi-square test. Results Statistically significant differences were found in the vertical marginal gap, where HPCs had the highest value, followed by ZRCs and SSCs ( P < 0.001); however, these values were all within clinically acceptable range. There was no statistically significant difference in surface roughness ( P > 0.016). SSCs presented the greatest amount of wear, followed by HPCs and ZRCs ( P < 0.001). Hybrid polymer-based crowns showed the greatest color change, followed by ZRCs ( P < 0.001). HPCs showed the greatest color change ( P < 0.001). SSCs had the highest fracture resistance (1713.00 ± 181.84 N), whereas HPCs (980.72 ± 132.41 N) and ZRCs (1039.63 ± 209.21 N) did not differ significantly. HPCs and SSCs exhibited surface deformation and microperforations, whereas ZRCs exhibited fracture. Conclusions HPCs, ZRCs, and SSCs had vertical marginal gap values within the clinically acceptable range, and no significant differences were found in surface roughness between groups. HPCs showed lower crown wear than SSCs and lower antagonist wear than ZRCs and SSCs. HPCs exhibited greater color change than ZRCs, while their fracture resistance was not significantly different from that of ZRCs.

BMC Oral Health
Cairo University (EG)
Cairo University
Good health and well-being
Dental materials and restorations
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon