Effects of Bamboo and Cocopeat-Based Cellulose Fibers on the Properties of Low-Carbon Mortar Containing Recycled Brick Aggregates

This study investigates a low-carbon mortar in which 60% of the Portland composite cement (PCC) was replaced by fly ash (40%), limestone powder (15%), and metakaolin (5%), reinforced with alkali-treated bamboo cellulose (CB) or cocopeat cellulose (CCP), and containing recycled brick aggregate (RA) as a 20% replacement for natural sand. First, the CB dosage was varied from 0.5% to 2% of binder mass in plain cement mortar; 1.5% gave the highest 28-day compressive strength (29.9 MPa versus 25.3 MPa for the control) and was adopted for the second stage. Compressive (7 and 28 days) and flexural (28 days) strengths were measured, and hydration and microstructure were examined by X-ray diffraction (XRD) and scanning electron microscopy with energy-dispersive spectroscopy (SEM-EDS). The pozzolanic binder and the cellulose reduced the 7-day compressive strength by up to 32%. XRD indicated that both celluloses retarded early clinker hydration but promoted carboaluminate formation by 28 days, when the fiber mixtures reached 17.2–17.4 MPa, versus 16.6 MPa for the plain pozzolan mortar and 20.0 MPa for the control. The fiber mixtures containing RA reached 20.0–20.1 MPa. Bamboo cellulose gave the highest flexural strength, 5.61 MPa, 31% above the control and 14% above the plain pozzolan mortar, and SEM showed intact bamboo fibers bridging pores, whereas cocopeat cellulose left it practically unchanged (4.98 versus 4.90 MPa). The load–displacement curves showed that bamboo cellulose raised both the peak load and the displacement at failure of the pozzolan mortar, consistent with microcrack bridging, although no mixture showed a post-peak softening branch. RA reduced the flexural strength of the bamboo and cocopeat mixtures by 33% and 28%, to 3.78 and 3.59 MPa, respectively, below that of the control. The bamboo cellulose mortar with RA therefore offers the best balance of clinker reduction, waste valorization, and strength, with flexural performance as the main limitation.

Authors

Institutions

Publication Details

Journal
Research Square
Published
2026-11-18
DOI
https://doi.org/10.21203/rs.3.rs-11576517/v1
Primary Topic
Concrete and Cement Materials Research
Type
preprint
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
preprint

Effects of Bamboo and Cocopeat-Based Cellulose Fibers on the Properties of Low-Carbon Mortar Containing Recycled Brick Aggregates

Henry Fonda Aritonang, Steve W.M. Supit, Debby Willar, Stefani Switly Peginusa et al.
2 links
Research Square
Concrete and Cement Materials Research
preprint

Effects of Bamboo and Cocopeat-Based Cellulose Fibers on the Properties of Low-Carbon Mortar Containing Recycled Brick Aggregates

Henry Fonda Aritonang, Steve W.M. Supit, Debby Willar, Stefani Switly Peginusa, Priyono Priyono
preprint en

Abstract

This study investigates a low-carbon mortar in which 60% of the Portland composite cement (PCC) was replaced by fly ash (40%), limestone powder (15%), and metakaolin (5%), reinforced with alkali-treated bamboo cellulose (CB) or cocopeat cellulose (CCP), and containing recycled brick aggregate (RA) as a 20% replacement for natural sand. First, the CB dosage was varied from 0.5% to 2% of binder mass in plain cement mortar; 1.5% gave the highest 28-day compressive strength (29.9 MPa versus 25.3 MPa for the control) and was adopted for the second stage. Compressive (7 and 28 days) and flexural (28 days) strengths were measured, and hydration and microstructure were examined by X-ray diffraction (XRD) and scanning electron microscopy with energy-dispersive spectroscopy (SEM-EDS). The pozzolanic binder and the cellulose reduced the 7-day compressive strength by up to 32%. XRD indicated that both celluloses retarded early clinker hydration but promoted carboaluminate formation by 28 days, when the fiber mixtures reached 17.2–17.4 MPa, versus 16.6 MPa for the plain pozzolan mortar and 20.0 MPa for the control. The fiber mixtures containing RA reached 20.0–20.1 MPa. Bamboo cellulose gave the highest flexural strength, 5.61 MPa, 31% above the control and 14% above the plain pozzolan mortar, and SEM showed intact bamboo fibers bridging pores, whereas cocopeat cellulose left it practically unchanged (4.98 versus 4.90 MPa). The load–displacement curves showed that bamboo cellulose raised both the peak load and the displacement at failure of the pozzolan mortar, consistent with microcrack bridging, although no mixture showed a post-peak softening branch. RA reduced the flexural strength of the bamboo and cocopeat mixtures by 33% and 28%, to 3.78 and 3.59 MPa, respectively, below that of the control. The bamboo cellulose mortar with RA therefore offers the best balance of clinker reduction, waste valorization, and strength, with flexural performance as the main limitation.

Research Square
Politeknik Negeri Manado (ID), Sam Ratulangi University (ID)
Responsible consumption and production, Industry, innovation and infrastructure
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.