Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination

Fissured rock masses in cold regions undergo matrix deterioration and structural weakening simultaneously, and separating the contribution of each remains difficult. Intact sandstone and parallel double-flawed sandstone with fissure inclinations of 30°, 45°, and 60° were therefore tested in uniaxial compression after 0, 10, 20, 30, and 50 freeze–thaw cycles, with digital image correlation (DIC), acoustic emission (AE), and scanning electron microscopy (SEM) linking macroscopic degradation to strain localization, crack activity, and microstructural change. Peak strength and apparent elastic modulus generally decreased with freeze–thaw cycling: after 50 cycles, the peak strength of intact specimens decreased from approximately 148 to 100 MPa, while the mean apparent elastic modulus of the 60° flawed group decreased from 13.14 to 6.49 GPa (49.36% retained). Freeze–thaw treatment altered the progressive development of surface strain localization and was associated with earlier AE activity, whereas fissure inclination influenced the spatial distribution of localized deformation and the resulting failure modes. Analysis based on the ratio of rise time to amplitude (RA) and average frequency (AF) showed a growing proportion of tensile cracking in every configuration; the 45° group shifted from 55.39% shear-dominated to 68.23% tensile-dominated. SEM images recorded progressive pore enlargement, interfacial debonding, and particle spalling. This study provides experimental evidence linking freeze–thaw-induced mechanical degradation with fissure inclination-dependent damage localization and fracture evolution in double-flawed sandstone. Freeze–thaw cycling thus sets the deterioration level of the material, while fissure inclination directs where and how failure develops.

Authors

Institutions

Publication Details

Journal
Applied Sciences
Published
2026-11-18
DOI
https://doi.org/10.3390/app162211442
Primary Topic
Rock Mechanics and Modeling
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination

Haiquan Wang, Lihai Tan, Min Yang, Song Jiang et al.
2 links
Applied Sciences
Rock Mechanics and Modeling
article

Mechanical Degradation and Damage Evolution of Double-Flawed Sandstone Under Freeze–Thaw Cycles: Effect of Fissure Inclination

Haiquan Wang, Lihai Tan, Min Yang, Song Jiang, Tao Xue, Zhao Wang, Haofei Liu
article en

Abstract

Fissured rock masses in cold regions undergo matrix deterioration and structural weakening simultaneously, and separating the contribution of each remains difficult. Intact sandstone and parallel double-flawed sandstone with fissure inclinations of 30°, 45°, and 60° were therefore tested in uniaxial compression after 0, 10, 20, 30, and 50 freeze–thaw cycles, with digital image correlation (DIC), acoustic emission (AE), and scanning electron microscopy (SEM) linking macroscopic degradation to strain localization, crack activity, and microstructural change. Peak strength and apparent elastic modulus generally decreased with freeze–thaw cycling: after 50 cycles, the peak strength of intact specimens decreased from approximately 148 to 100 MPa, while the mean apparent elastic modulus of the 60° flawed group decreased from 13.14 to 6.49 GPa (49.36% retained). Freeze–thaw treatment altered the progressive development of surface strain localization and was associated with earlier AE activity, whereas fissure inclination influenced the spatial distribution of localized deformation and the resulting failure modes. Analysis based on the ratio of rise time to amplitude (RA) and average frequency (AF) showed a growing proportion of tensile cracking in every configuration; the 45° group shifted from 55.39% shear-dominated to 68.23% tensile-dominated. SEM images recorded progressive pore enlargement, interfacial debonding, and particle spalling. This study provides experimental evidence linking freeze–thaw-induced mechanical degradation with fissure inclination-dependent damage localization and fracture evolution in double-flawed sandstone. Freeze–thaw cycling thus sets the deterioration level of the material, while fissure inclination directs where and how failure develops.

Applied SciencesVol. 16(22)
Xi'an University of Architecture and Technology (CN), University of South China (CN)
National Natural Science Foundation of China
Rock Mechanics and Modeling
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon