Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric Liners

Abstract Polymeric materials are increasingly used in natural gas infrastructure, yet their long-term reliability under realistic service conditions remains poorly characterized, particularly in the presence of potential reactive contaminants. In this work, we investigate the aging behavior of high-density polyethylene (HDPE), nylon-6/6 polyamide (PA), and poly(vinylidene fluoride) (PVDF) exposed to a natural gas mixture containing 0.5% oxygen as a model reactive contaminant. Using dynamic mechanical analysis (DMA), time–temperature superposition (TTS), and Fourier-transform infrared spectroscopy (FTIR), we characterize the evolution of mechanical properties, viscoelastic relaxation dynamics, and chemical structure under accelerated aging conditions with elevated temperature and pressure. While conventional mechanical properties provide ambiguous and often noisy metrics, we observe a pronounced reduction in the activation energy Ea associated with segmental relaxation across all polymers, indicating accelerated molecular dynamics. The presence of oxygen significantly enhances this effect, particularly at early aging times. We classify the aging response based on whether activation energy Ea recovers after the polymer is removed from the gas environment. For HDPE, PVDF, and PA samples aged at room temperature, the decrease in Ea recovers almost entirely once the polymers are removed from the natural gas environment, consistent with physical absorption. By contrast, PA samples aged at 90 °C exhibit only partial recovery of mechanical properties and persistent FTIR features, indicating chemical changes induced by the oxygenated environment. These results demonstrate that viscoelastic measurements can distinguish between reversible and irreversible degradation processes that may not be detected by conventional measurements.

Authors

Institutions

Publication Details

Journal
ACS Applied Polymer Materials
Published
2026-11-17
DOI
https://doi.org/10.1021/acsapm.6c03876
Primary Topic
Material Properties and Failure Mechanisms
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric Liners

Ryan Poling‐Skutvik, Edith Mathiowitz, Vikas Srivastava, Keven Alkhoury et al.
1 links
ACS Applied Polymer Materials
Material Properties and Failure Mechanisms
article

Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric Liners

Ryan Poling‐Skutvik, Edith Mathiowitz, Vikas Srivastava, Keven Alkhoury, Zakhar Lyakhovych, Mohammadjavad Haji Rezaei, Deepro Ghosh
article en

Abstract

Abstract Polymeric materials are increasingly used in natural gas infrastructure, yet their long-term reliability under realistic service conditions remains poorly characterized, particularly in the presence of potential reactive contaminants. In this work, we investigate the aging behavior of high-density polyethylene (HDPE), nylon-6/6 polyamide (PA), and poly(vinylidene fluoride) (PVDF) exposed to a natural gas mixture containing 0.5% oxygen as a model reactive contaminant. Using dynamic mechanical analysis (DMA), time–temperature superposition (TTS), and Fourier-transform infrared spectroscopy (FTIR), we characterize the evolution of mechanical properties, viscoelastic relaxation dynamics, and chemical structure under accelerated aging conditions with elevated temperature and pressure. While conventional mechanical properties provide ambiguous and often noisy metrics, we observe a pronounced reduction in the activation energy Ea associated with segmental relaxation across all polymers, indicating accelerated molecular dynamics. The presence of oxygen significantly enhances this effect, particularly at early aging times. We classify the aging response based on whether activation energy Ea recovers after the polymer is removed from the gas environment. For HDPE, PVDF, and PA samples aged at room temperature, the decrease in Ea recovers almost entirely once the polymers are removed from the natural gas environment, consistent with physical absorption. By contrast, PA samples aged at 90 °C exhibit only partial recovery of mechanical properties and persistent FTIR features, indicating chemical changes induced by the oxygenated environment. These results demonstrate that viscoelastic measurements can distinguish between reversible and irreversible degradation processes that may not be detected by conventional measurements.

ACS Applied Polymer Materials
University of Rhode Island (US), Brown University (US)
U.S. Department of Transportation, Pipeline and Hazardous Materials Safety Administration
Material Properties and Failure Mechanisms
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon