Source-Dependent Performance of Calcium Silicate-Based Co-Products Derived from Phosphoric Acid Production Processes
The phosphate fertilizer industry generates large quantities of phosphogypsum, motivating beneficial-use pathways that convert phosphate-industry residuals into construction materials. This study evaluated calcium silicate-rich J-Rox co-products produced through two source routes: phosphate ore-derived J-Rox from the phosphoric acid production route (JR-P) and phosphogypsum-derived J-Rox from the phosphogypsum recovery route (JR-G). Finely ground J-Rox was examined as a supplementary cementitious material through a staged paste–mortar–concrete framework, while coarsely ground phosphogypsum-derived J-Rox sand was evaluated as a prewetted internal curing aggregate. Paste testing assessed setting behavior, mortar testing evaluated workability-controlled compressive strength and sulfate attack resistance, and concrete testing validated JR-G materials (JR-G1 and JR-G2) in binary, ternary J-Rox–slag, and internally cured systems. JR-P materials produced more systematic setting delay, likely influenced by higher P2O5 contents, while JR-G materials showed more variable but practical setting behavior. Mortar strength results were material- and dosage-dependent, with 15% replacement giving the most consistent response. Sulfate expansion provided the clearest source-route distinction: all JR-G mixtures remained below the 0.1% expansion threshold at 26 weeks, with an average expansion of 0.0560%, while five of the six JR-P mixtures exceeded this threshold, with an average expansion of 0.1499%. At the concrete scale, binary JR-G mixtures achieved practical 28-day strength, with the 15JR-G2 mixture reaching 7593 psi at 91 days compared with 6694 psi for the OPC control. Ternary mixtures containing 15% JR-G and 35% slag showed strong later-age strength gain, increased surface resistivity, and reduced drying shrinkage at 50% OPC replacement. Specifically, the 15JR-G2/35S mixture achieved a 91-day compressive strength of 7372 psi, while the 15JR-G1/35S mixture exhibited a 112-day drying shrinkage of −0.011%, compared with −0.066% for the OPC control. These results indicate that phosphogypsum-derived J-Rox use in concrete materials shows promise, particularly when used in ternary, performance-engineered blended binder systems.
Authors
- Brett Q. Tempest (ORCID: https://orcid.org/0000-0001-6096-4520)
- Jamshid M. Armaghani
- Tara L. Cavalline (ORCID: https://orcid.org/0000-0002-4745-1920)
- Mark Vignovic
- Clarke J. Summers
- Shubham Mishra
- Samantha R. Doughty
Institutions
- University of North Carolina at Charlotte (US)
- University of Southern Indiana (US)
- Novaphos (United States) (US)
Publication Details
- Journal
- Construction Materials
- Published
- 2026-11-17
- DOI
- https://doi.org/10.3390/constrmater6060107
- Primary Topic
- Concrete and Cement Materials Research
- Type
- article
- Field-Weighted Citation Impact
- 0.00