Structure–Property Tailoring of Long-Chain PDMS-Based Polyurethanes for Flexible MXene Strain Sensors

Flexible and mechanically adaptable polymer substrates are critical for conformable wearable sensors capable of accurately tracking human motion and vital parameters. Here, crosslinked polyurethanes (PUs) were synthesized from a long-chain poly(ethylene oxide)-b-poly(dimethylsiloxane)-b-poly(ethylene oxide) (PEO–PDMS–PEO) macrodiol (Mn = 2400 g mol−1), 4,4′-methylenediphenyl diisocyanate, and a multifunctional hyperbranched polyester, with soft-segment contents of 15–70 wt.%. Mechanical, structural, surface, and thermal properties were evaluated by indentation methods (nanoindentation, microindentation, and microindentation creep), XRD, AFM, wettability measurements, TGA, and DSC. Increasing the soft-segment content markedly reduced stiffness; Young’s modulus decreased from 1713 MPa to 112 MPa to 80 MPa as the soft segment content was increased from 30 wt.% to 50 wt.% to 70 wt.%, respectively, while hardness decreased from 89 to 4 MPa. The predominantly amorphous networks retained good thermal stability, with degradation temperature (T(10%)) values of 249–291 °C and glass transition temperature (Tg) values of 21–25 °C. Increasing the soft-segment content also increased surface roughness (Rq: 18.3–250 nm) and water contact angle (approximately 45–90°), indicating progressive surface enrichment by the low-surface-energy PDMS-containing phase. PU-50 was selected as the finger-motion sensor substrate and coated with Ti3C2Tx MXene by spray deposition. The MXene/PU-50 sensor exhibited a gauge factor of 65.9 over 0–8% strain, response/recovery times of 138/58 ms, and a signal-to-noise ratio (SNR) of 39.5 dB, demonstrating a reversible piezoresistive response with good short-term repeatability and the feasibility of using a long-chain PDMS-based PU substrate for rapid and sensitive wearable strain sensing.

Authors

Institutions

Publication Details

Journal
Materials
Published
2026-11-17
DOI
https://doi.org/10.3390/ma19224861
Primary Topic
Advanced Sensor and Energy Harvesting Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Structure–Property Tailoring of Long-Chain PDMS-Based Polyurethanes for Flexible MXene Strain Sensors

Dana G. Vasiljević-Radović, Marko Spasenović, Marija V. Pergal, Darko M. Micic et al.
1 links
Materials
Advanced Sensor and Energy Harvesting Materials
article

Structure–Property Tailoring of Long-Chain PDMS-Based Polyurethanes for Flexible MXene Strain Sensors

Dana G. Vasiljević-Radović, Marko Spasenović, Marija V. Pergal, Darko M. Micic, Milena Rašljić Rafajilović, Ivan Pešić, Zdravko Džambaski, Ivana O. Mladenović, Aleksa Bakoč
article en

Abstract

Flexible and mechanically adaptable polymer substrates are critical for conformable wearable sensors capable of accurately tracking human motion and vital parameters. Here, crosslinked polyurethanes (PUs) were synthesized from a long-chain poly(ethylene oxide)-b-poly(dimethylsiloxane)-b-poly(ethylene oxide) (PEO–PDMS–PEO) macrodiol (Mn = 2400 g mol−1), 4,4′-methylenediphenyl diisocyanate, and a multifunctional hyperbranched polyester, with soft-segment contents of 15–70 wt.%. Mechanical, structural, surface, and thermal properties were evaluated by indentation methods (nanoindentation, microindentation, and microindentation creep), XRD, AFM, wettability measurements, TGA, and DSC. Increasing the soft-segment content markedly reduced stiffness; Young’s modulus decreased from 1713 MPa to 112 MPa to 80 MPa as the soft segment content was increased from 30 wt.% to 50 wt.% to 70 wt.%, respectively, while hardness decreased from 89 to 4 MPa. The predominantly amorphous networks retained good thermal stability, with degradation temperature (T(10%)) values of 249–291 °C and glass transition temperature (Tg) values of 21–25 °C. Increasing the soft-segment content also increased surface roughness (Rq: 18.3–250 nm) and water contact angle (approximately 45–90°), indicating progressive surface enrichment by the low-surface-energy PDMS-containing phase. PU-50 was selected as the finger-motion sensor substrate and coated with Ti3C2Tx MXene by spray deposition. The MXene/PU-50 sensor exhibited a gauge factor of 65.9 over 0–8% strain, response/recovery times of 138/58 ms, and a signal-to-noise ratio (SNR) of 39.5 dB, demonstrating a reversible piezoresistive response with good short-term repeatability and the feasibility of using a long-chain PDMS-based PU substrate for rapid and sensitive wearable strain sensing.

MaterialsVol. 19(22)
University of Belgrade (RS), Institute of General and Physical Chemistry (RS), Institute of Chemistry, Technology and Metallurgy (RS)
Science Fund of the Republic of Serbia
Advanced Sensor and Energy Harvesting Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon