Effect of die-exit argon-gas cooling on microstructure, texture, mechanical properties, and in vitro degradation behavior of extruded Mg–Zn–Mn–Sr microtubes

Mg alloy microtubes for bioresorbable vascular stents require dimensional accuracy, adequate room-temperature tensile properties, and predictable degradation behavior. In this study, Mg–1.07Zn–0.49Mn–0.52Sr (wt%) alloy microtubes were fabricated by two-step direct extrusion without (NC) and with die-exit argon-gas cooling (AGC). Both conditions produced microtubes with an outer diameter of approximately 2.1 mm and a wall thickness close to 0.20 mm. AGC modified the monitored subsurface near-exit die-temperature history, but the measurements neither quantified microtube cooling rates nor isolated post-exit cooling. Across three EBSD maps of the same specimen per condition, AGC reduced the mean area-weighted grain diameter from 9.2 ± 0.2 µm to 5.1 ± 0.1 µm (mean ± SD of map-level values), a reduction of approximately 44%. The area fraction of high grain orientation spread (GOS ≥ 1°) increased from 4.7 ± 2.1% to 10.0 ± 0.8%. Both conditions retained a dominant extrusion-related texture, with similar mean Schmid factors for basal and prismatic 〈a〉 slip. AGC increased the tensile yield strength from 197 ± 1 MPa to 227 ± 1 MPa and the ultimate tensile strength from 243 ± 3 MPa to 265 ± 1 MPa. Elongation was 8.7 ± 1.2% for NC and 8.5 ± 0.8% for AGC; ductility equivalence was not established with three specimens per condition. Work-hardening analysis using effective true stress suggested a higher initial flow stress in AGC without enhanced post-yield hardening. Seven-day hydrogen-evolution and mass-loss measurements did not resolve a difference between NC and AGC (n = 3 per condition), and the electrochemical responses showed no persistent separation. AGC was associated with a finer as-extruded microstructure and higher axial tensile strength, while the short-term degradation behavior did not establish equivalence between conditions.

Authors

Institutions

Publication Details

Journal
Journal of Magnesium and Alloys
Published
2026-11-17
DOI
https://doi.org/10.1016/j.jma.2026.102399
Primary Topic
Magnesium Alloys: Properties and Applications
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effect of die-exit argon-gas cooling on microstructure, texture, mechanical properties, and in vitro degradation behavior of extruded Mg–Zn–Mn–Sr microtubes

Joung Sik Suh, Ha Sik Kim, Sang Eun Lee, Jae-Yeon Kim et al.
Journal of Magnesium and Alloys
Magnesium Alloys: Properties and Applications
article

Effect of die-exit argon-gas cooling on microstructure, texture, mechanical properties, and in vitro degradation behavior of extruded Mg–Zn–Mn–Sr microtubes

Joung Sik Suh, Ha Sik Kim, Sang Eun Lee, Jae-Yeon Kim, Minseo Lee, Geonho Hwang
article en

Abstract

Mg alloy microtubes for bioresorbable vascular stents require dimensional accuracy, adequate room-temperature tensile properties, and predictable degradation behavior. In this study, Mg–1.07Zn–0.49Mn–0.52Sr (wt%) alloy microtubes were fabricated by two-step direct extrusion without (NC) and with die-exit argon-gas cooling (AGC). Both conditions produced microtubes with an outer diameter of approximately 2.1 mm and a wall thickness close to 0.20 mm. AGC modified the monitored subsurface near-exit die-temperature history, but the measurements neither quantified microtube cooling rates nor isolated post-exit cooling. Across three EBSD maps of the same specimen per condition, AGC reduced the mean area-weighted grain diameter from 9.2 ± 0.2 µm to 5.1 ± 0.1 µm (mean ± SD of map-level values), a reduction of approximately 44%. The area fraction of high grain orientation spread (GOS ≥ 1°) increased from 4.7 ± 2.1% to 10.0 ± 0.8%. Both conditions retained a dominant extrusion-related texture, with similar mean Schmid factors for basal and prismatic 〈a〉 slip. AGC increased the tensile yield strength from 197 ± 1 MPa to 227 ± 1 MPa and the ultimate tensile strength from 243 ± 3 MPa to 265 ± 1 MPa. Elongation was 8.7 ± 1.2% for NC and 8.5 ± 0.8% for AGC; ductility equivalence was not established with three specimens per condition. Work-hardening analysis using effective true stress suggested a higher initial flow stress in AGC without enhanced post-yield hardening. Seven-day hydrogen-evolution and mass-loss measurements did not resolve a difference between NC and AGC (n = 3 per condition), and the electrochemical responses showed no persistent separation. AGC was associated with a finer as-extruded microstructure and higher axial tensile strength, while the short-term degradation behavior did not establish equivalence between conditions.

Journal of Magnesium and AlloysVol. 26
Korea University (KR), Korea Institute of Materials Science (KR)
National Research Foundation of Korea, Ministry of Science and ICT, South Korea
Magnesium Alloys: Properties and Applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon