Metal-semiconductor field effect transistors based on zinc nitride/zinc oxide interface deposited at room temperature

Abstract In this work, bottom-gate top-contact zinc nitride/zinc oxide (Zn3N2/ZnO) metal-semiconductor field-effect transistors (MESFETs) are presented. Palladium is used as Schottky gate contact, while aluminum is used as ohmic source/drain contacts. ZnO is used as passivation film. The Zn3N2 and ZnO thin films are deposited at room temperature by radio frequency magnetron sputtering. The ohmic Al/Zn3N2 contacts were analyzed by the transmission line method. Interestingly, the Zn3N2/ZnO MESFETs exhibit a “normally-off” p-type behavior. A possible explanation is an unintentional p-type ZnO:N interlayer film formed at the Zn3N2/ZnO interface. The elemental profile at the ZnO/ Zn3N2 interface revealed an oxygen–nitrogen compositional balance, providing evidence for the possible formation of the ZnO:N interlayer. The device exhibits an ION/IOFF current ratio higher than 103, an off-current ~10-8 A (~10-14 A/cm), a threshold voltage VT ~0.35 V, a maximum transconductance ~1.42 × 10-5 A/V, and a subthreshold slope of 98 mV/Dec.

Authors

Institutions

Publication Details

Journal
Semiconductor Science and Technology
Published
2026-11-17
DOI
https://doi.org/10.1088/1361-6641/aec320
Primary Topic
ZnO doping and properties
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Metal-semiconductor field effect transistors based on zinc nitride/zinc oxide interface deposited at room temperature

Andrés Redondo‐Cubero, Miguel A. Domínguez
Semiconductor Science and Technology
ZnO doping and properties
article

Metal-semiconductor field effect transistors based on zinc nitride/zinc oxide interface deposited at room temperature

Andrés Redondo‐Cubero, Miguel A. Domínguez
article en

Abstract

Abstract In this work, bottom-gate top-contact zinc nitride/zinc oxide (Zn3N2/ZnO) metal-semiconductor field-effect transistors (MESFETs) are presented. Palladium is used as Schottky gate contact, while aluminum is used as ohmic source/drain contacts. ZnO is used as passivation film. The Zn3N2 and ZnO thin films are deposited at room temperature by radio frequency magnetron sputtering. The ohmic Al/Zn3N2 contacts were analyzed by the transmission line method. Interestingly, the Zn3N2/ZnO MESFETs exhibit a “normally-off” p-type behavior. A possible explanation is an unintentional p-type ZnO:N interlayer film formed at the Zn3N2/ZnO interface. The elemental profile at the ZnO/ Zn3N2 interface revealed an oxygen–nitrogen compositional balance, providing evidence for the possible formation of the ZnO:N interlayer. The device exhibits an ION/IOFF current ratio higher than 103, an off-current ~10-8 A (~10-14 A/cm), a threshold voltage VT ~0.35 V, a maximum transconductance ~1.42 × 10-5 A/V, and a subthreshold slope of 98 mV/Dec.

Semiconductor Science and Technology
Universidad Autónoma de Madrid (ES), Benemérita Universidad Autónoma de Puebla (MX)
Fundación Carolina
ZnO doping and properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon