Reinforcement Corrosion in Coral Aggregate Concrete: 20-Month In-Situ Comparison of Portland, Magnesium Phosphate, and Hybrid Fly Ash–Silica Fume Binders in the South China Sea

Reinforcement corrosion is a governing durability concern for coral aggregate concrete (CAC) structures in the South China Sea, yet long-term field evidence comparing alternative binder systems under natural marine exposure remains scarce. This study reports a 20-month in-situ exposure campaign on a natural reef-flat platform in Zhanjiang Bay, in which HRB400 carbon steel and 316L stainless steel rebars were embedded in CAC prepared with Portland cement (PC), magnesium phosphate cement (MPC), and a hybrid fly ash–silica fume binder (HF) at a fixed water-to-binder ratio of 0.30. Open-circuit potential was monitored over early (0–5 months), middle (5–12 months), and late (12–20 months) exposure windows, and potentiodynamic polarization was measured at three snapshot ages (month 5; months 12–14; months 19–20), complemented by rapid chloride migration testing, XRD, and SEM–EDS. The corrosion behavior of carbon steel was strongly binder-dependent. In the MPC matrix, carbon steel underwent severe early-stage activation (icorr = 7.92 µA/cm2, equivalent to 91.9 µm/y), which is attributed to the near-neutral pore solution of the portlandite-free K-struvite matrix; the corrosion rate subsequently decreased by more than four orders of magnitude, a trend consistent with a transition toward transport-limited kinetics rather than a restoration of passivity. The HF binder yielded the lowest chloride migration coefficient (0.171 × 10−12 m2/s) and sustained low corrosion rates of carbon steel, plausibly reflecting pozzolanic pore refinement and chloride binding. 316L stainless steel remained below the RILEM TC 154-EMC passivity threshold (0.1 µA/cm2) in all three binders. These results suggest that binder–reinforcement compatibility, rather than matrix density alone, governs the long-term corrosion performance of CAC in reef-flat environments.

Authors

Institutions

Publication Details

Journal
Journal of Marine Science and Engineering
Published
2026-11-17
DOI
https://doi.org/10.3390/jmse14222181
Primary Topic
Concrete Corrosion and Durability
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Reinforcement Corrosion in Coral Aggregate Concrete: 20-Month In-Situ Comparison of Portland, Magnesium Phosphate, and Hybrid Fly Ash–Silica Fume Binders in the South China Sea

林细炳, Dapeng Zhang, Li Yating, Qinghua Li et al.
1 links
Journal of Marine Science and Engineering
Concrete Corrosion and Durability
article

Reinforcement Corrosion in Coral Aggregate Concrete: 20-Month In-Situ Comparison of Portland, Magnesium Phosphate, and Hybrid Fly Ash–Silica Fume Binders in the South China Sea

林细炳, Dapeng Zhang, Li Yating, Qinghua Li, Huiling Zhang
article en

Abstract

Reinforcement corrosion is a governing durability concern for coral aggregate concrete (CAC) structures in the South China Sea, yet long-term field evidence comparing alternative binder systems under natural marine exposure remains scarce. This study reports a 20-month in-situ exposure campaign on a natural reef-flat platform in Zhanjiang Bay, in which HRB400 carbon steel and 316L stainless steel rebars were embedded in CAC prepared with Portland cement (PC), magnesium phosphate cement (MPC), and a hybrid fly ash–silica fume binder (HF) at a fixed water-to-binder ratio of 0.30. Open-circuit potential was monitored over early (0–5 months), middle (5–12 months), and late (12–20 months) exposure windows, and potentiodynamic polarization was measured at three snapshot ages (month 5; months 12–14; months 19–20), complemented by rapid chloride migration testing, XRD, and SEM–EDS. The corrosion behavior of carbon steel was strongly binder-dependent. In the MPC matrix, carbon steel underwent severe early-stage activation (icorr = 7.92 µA/cm2, equivalent to 91.9 µm/y), which is attributed to the near-neutral pore solution of the portlandite-free K-struvite matrix; the corrosion rate subsequently decreased by more than four orders of magnitude, a trend consistent with a transition toward transport-limited kinetics rather than a restoration of passivity. The HF binder yielded the lowest chloride migration coefficient (0.171 × 10−12 m2/s) and sustained low corrosion rates of carbon steel, plausibly reflecting pozzolanic pore refinement and chloride binding. 316L stainless steel remained below the RILEM TC 154-EMC passivity threshold (0.1 µA/cm2) in all three binders. These results suggest that binder–reinforcement compatibility, rather than matrix density alone, governs the long-term corrosion performance of CAC in reef-flat environments.

Journal of Marine Science and EngineeringVol. 14(22)
Guangdong Ocean University (CN)
Concrete Corrosion and Durability
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon