Influence of High Temperature on Cycling and Calendar Degradation of Lithium-Ion Batteries with Thermal Changes
The aging mechanism and safety revolution of lithium-ion batteries (LIBs) are always influenced by the working temperature. The degradation path and thermal characteristics of LIBs at high temperature were investigated both from the aspect of cycle aging and calendar aging in this study. High temperature (55 °C) with temperature rate, cycle number, calendar time, and charging/discharging rate were taken into consideration to validate the battery performance under dynamic operating conditions. The basic electrochemical index, including capacity loss, internal resistance growth, and incremental capacity curve (IC curve) of LIBs, was first analyzed. Then, capacity loss and internal resistance growth were calculated both under cycling and calendar conditions with high temperature. Thermal characteristics were further analyzed by entropy change, enthalpy change, and temperature rate during the high-temperature cycling. Moreover, adiabatic thermal experimental results under 0% state of charge (SOC) were also conducted for further safety analysis. A non-monotonic calendar-aging maximum near 75% SOC and a rate-dependent degradation minimum at intermediate rates were identified. The aging and calendar laws of LIBs at high temperature and high rate were then concluded as reference to support the usage management and storage strategies of LIBs.
Authors
- Bing Xue (ORCID: https://orcid.org/0000-0001-6740-4665)
- Ruiheng Wang
Institutions
- Changzhou University (CN)
Publication Details
- Journal
- Batteries
- Published
- 2026-11-17
- DOI
- https://doi.org/10.3390/batteries12110496
- Primary Topic
- Battery Modeling and Management
- Type
- article
- Field-Weighted Citation Impact
- 0.00