Studi Eksperimental Zeolit sebagai Pengganti Sebagian Semen terhadap Kuat Tekan Self-Compacting Concrete (SCC)

This study aims to evaluate the mix design, fresh concrete properties, and compressive strength development of Self-Compacting Concrete (SCC) utilizing natural zeolite as a partial cement replacement. The zeolite substitution ratios were set at 0%, 5%, 10%, 12.5%, and 15% by weight of cement, targeting a specified compressive strength of 45 MPa at 28 days. The mix proportions were developed based on SNI 03-6468-2000 in conjunction with Okamura's method and Bina Marga SKh.1.7.23 specifications. Slump flow tests were conducted to determine fresh workability, while compressive strength tests on 10x20 cm cylindrical specimens were performed at ages of 7, 14, and 28 days. The results revealed that increasing zeolite content reduced slump flow due to the higher water absorption and specific surface area of zeolite particles. The mixtures with 0%, 5%, and 10% zeolite achieved slump flow values of 60 cm, 58 cm, and 58 cm, respectively, complying with the EFNARC Class SF1 criteria. Conversely, the 12.5% and 15% mixtures failed to meet the flowability thresholds. Regarding hardened properties, the 10% zeolite replacement yielded optimum mechanical performance, achieving a 28-day compressive strength of 42.43 MPa (a 4.05% increase compared to the 40.78 MPa control). Exceeding 10% zeolite replacement caused strength degradation due to the reduction of primary cementitious binder. Fracture behavior evaluation confirmed normal failure modes (cone, cone and split, cone and shear) across all test specimens. In conclusion, a 10% zeolite replacement ratio is identified as the optimum dosage that balances optimal workability and compressive strength in SCC.

Authors

Institutions

Publication Details

Journal
Jurnal MESIL (Mesin Elektro Sipil)
Published
2026-11-18
DOI
https://doi.org/10.53695/jm.v7i2.1721
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Studi Eksperimental Zeolit sebagai Pengganti Sebagian Semen terhadap Kuat Tekan Self-Compacting Concrete (SCC)

A Shakira, E Widyaningsih
2 links
Jurnal MESIL (Mesin Elektro Sipil)
Concrete and Cement Materials Research
article

Studi Eksperimental Zeolit sebagai Pengganti Sebagian Semen terhadap Kuat Tekan Self-Compacting Concrete (SCC)

A Shakira, E Widyaningsih
article en

Abstract

This study aims to evaluate the mix design, fresh concrete properties, and compressive strength development of Self-Compacting Concrete (SCC) utilizing natural zeolite as a partial cement replacement. The zeolite substitution ratios were set at 0%, 5%, 10%, 12.5%, and 15% by weight of cement, targeting a specified compressive strength of 45 MPa at 28 days. The mix proportions were developed based on SNI 03-6468-2000 in conjunction with Okamura's method and Bina Marga SKh.1.7.23 specifications. Slump flow tests were conducted to determine fresh workability, while compressive strength tests on 10x20 cm cylindrical specimens were performed at ages of 7, 14, and 28 days. The results revealed that increasing zeolite content reduced slump flow due to the higher water absorption and specific surface area of zeolite particles. The mixtures with 0%, 5%, and 10% zeolite achieved slump flow values of 60 cm, 58 cm, and 58 cm, respectively, complying with the EFNARC Class SF1 criteria. Conversely, the 12.5% and 15% mixtures failed to meet the flowability thresholds. Regarding hardened properties, the 10% zeolite replacement yielded optimum mechanical performance, achieving a 28-day compressive strength of 42.43 MPa (a 4.05% increase compared to the 40.78 MPa control). Exceeding 10% zeolite replacement caused strength degradation due to the reduction of primary cementitious binder. Fracture behavior evaluation confirmed normal failure modes (cone, cone and split, cone and shear) across all test specimens. In conclusion, a 10% zeolite replacement ratio is identified as the optimum dosage that balances optimal workability and compressive strength in SCC.

Jurnal MESIL (Mesin Elektro Sipil)Vol. 7(2)
Institut Teknologi Nasional Bandung (ID)
Responsible consumption and production, Industry, innovation and infrastructure
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.