Multi-scale and multi-technique characterization of a new ultra-fine ground glass pozzolan as a high content supplementary cementitious material

The carbon intensity of cement production and the declining supply of conventional supplementary cementitious materials (SCMs), driven by the phasing out of coal-fired electricity and the transition to electric furnace steelmaking, necessitate the identification of viable alternative SCMs. Whereas ground glass pozzolan (GGP) has emerged as a promising candidate, most existing applications are limited to around 20% replacement of cement, with higher replacement levels adversely affecting the development of mechanical strength—predominantly controlled by GGP particle size, which can limit or enhance reactivity. Herein, a novel ultra-fine ground glass pozzolan ( uf -GGP) with a median particle size (D 50 ) of 4.16 µm—more than three times finer than conventional GGP (D 50 ≈ 15 µm)—is investigated as an SCM at cement replacement levels up to 50% by mass, extending well beyond the 20% range in the mainstream literature. A multi-technique characterization approach was implemented on: ( i ) cement mortars (compressive strength and electrical resistivity, considering both the standard ASTM mixing method and a high-shear mixing method) and (ii) pastes (microstructural characterization and analysis, including thermogravimetry, X-ray diffraction, scanning electron microscopy with energy-dispersive spectroscopy, and thermodynamic modelling). Results show that clinker-dilution-related early-age compressive strength losses in uf -GGP mortars are progressively recovered through pozzolanic reaction, with 20–40% cement replacement significantly exceeding the control (0% replacement) at 91 days under high-shear mixing, which was found to be critical at high uf -GGP contents, while under ASTM mixing the optimal range was limited to 20–30%. The best overall performance was achieved at 40% uf -GGP using high-shear mixing, combining a 91-day compressive strength about 8% above that of the control with an approximately 16 times increase in electrical resistivity, which increased further, up to 30 times that of the control, at 50% uf -GGP, consistent with a refinement of the pore structure. Thermodynamic modelling of uf -GGP pastes indicated an uf -GGP content threshold between 40% and 50% cement replacement, beyond which complete portlandite consumption is predicted to cause strätlingite formation, constraining C–S–H production and limiting further compressive strength development. A simplified environmental assessment showed that 50% uf -GGP reduced the embodied CO 2 of the mortar by 46%, despite the observation that the embodied energy decreased by only 7% due to the grinding energy needed to produce the ultra-fine powder. Overall, uf -GGP could allow cement replacement levels well beyond those currently achievable with conventional GGP, which should be confirmed at the concrete scale .

Authors

Institutions

Publication Details

Journal
Construction and Building Materials
Published
2026-11-17
DOI
https://doi.org/10.1016/j.conbuildmat.2026.148874
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Multi-scale and multi-technique characterization of a new ultra-fine ground glass pozzolan as a high content supplementary cementitious material

Mahipal Kasaniya, Ousmane A. Hisseine, Ayman Mdallal
1 links
Construction and Building Materials
Concrete and Cement Materials Research
article

Multi-scale and multi-technique characterization of a new ultra-fine ground glass pozzolan as a high content supplementary cementitious material

Mahipal Kasaniya, Ousmane A. Hisseine, Ayman Mdallal
article en

Abstract

The carbon intensity of cement production and the declining supply of conventional supplementary cementitious materials (SCMs), driven by the phasing out of coal-fired electricity and the transition to electric furnace steelmaking, necessitate the identification of viable alternative SCMs. Whereas ground glass pozzolan (GGP) has emerged as a promising candidate, most existing applications are limited to around 20% replacement of cement, with higher replacement levels adversely affecting the development of mechanical strength—predominantly controlled by GGP particle size, which can limit or enhance reactivity. Herein, a novel ultra-fine ground glass pozzolan ( uf -GGP) with a median particle size (D 50 ) of 4.16 µm—more than three times finer than conventional GGP (D 50 ≈ 15 µm)—is investigated as an SCM at cement replacement levels up to 50% by mass, extending well beyond the 20% range in the mainstream literature. A multi-technique characterization approach was implemented on: ( i ) cement mortars (compressive strength and electrical resistivity, considering both the standard ASTM mixing method and a high-shear mixing method) and (ii) pastes (microstructural characterization and analysis, including thermogravimetry, X-ray diffraction, scanning electron microscopy with energy-dispersive spectroscopy, and thermodynamic modelling). Results show that clinker-dilution-related early-age compressive strength losses in uf -GGP mortars are progressively recovered through pozzolanic reaction, with 20–40% cement replacement significantly exceeding the control (0% replacement) at 91 days under high-shear mixing, which was found to be critical at high uf -GGP contents, while under ASTM mixing the optimal range was limited to 20–30%. The best overall performance was achieved at 40% uf -GGP using high-shear mixing, combining a 91-day compressive strength about 8% above that of the control with an approximately 16 times increase in electrical resistivity, which increased further, up to 30 times that of the control, at 50% uf -GGP, consistent with a refinement of the pore structure. Thermodynamic modelling of uf -GGP pastes indicated an uf -GGP content threshold between 40% and 50% cement replacement, beyond which complete portlandite consumption is predicted to cause strätlingite formation, constraining C–S–H production and limiting further compressive strength development. A simplified environmental assessment showed that 50% uf -GGP reduced the embodied CO 2 of the mortar by 46%, despite the observation that the embodied energy decreased by only 7% due to the grinding energy needed to produce the ultra-fine powder. Overall, uf -GGP could allow cement replacement levels well beyond those currently achievable with conventional GGP, which should be confirmed at the concrete scale .

Construction and Building MaterialsVol. 551
McMaster University (CA)
McMaster University, Natural Sciences and Engineering Research Council of Canada
Responsible consumption and production
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.