Development and Field Performance of a High-Visibility Thermoplastic Road Marking Formulation

Thermoplastic road marking coatings are composed of a resin binder, inorganic fillers, titanium dioxide pigment, glass beads, and functional additives. The proportioning of these components determines the mechanical durability, thermal stability, and optical performance of the coating, yet systematic formulation studies remain limited. This study developed a high-visibility thermoplastic road marking formulation through a single-factor experimental approach to address the common durability problems of thermal deformation and rapid retroreflectivity loss under heavy traffic and high-temperature conditions. The investigation quantitatively evaluated the effects of premixed glass bead dosage, the mass ratio of quartz sand to calcium carbonate filler, and titanium dioxide pigment content on the mechanical strength, thermal resistance, and optical performance of the coating. The experimental results demonstrated that a premixed glass bead content ranging from 31% to 33% provided the best combination of wear resistance and compressive strength. Regarding the filler composition, a quartz sand fraction of 6% to 7% formed a rigid skeletal network that effectively improved thermal deformation resistance and maintained compressive strength at 60℃. For optical performance, a rutile titanium dioxide dosage of 4.5% to 5.5% met the luminance factor requirements while avoiding the diminishing returns caused by particle agglomeration at higher concentrations. The optimized formulation, which employed a simplified additive system consisting solely of polyethylene wax and dioctyl phthalate plasticizer, was applied in a highway maintenance project with drop-on glass beads. Six months of field tracking showed that the initial retroreflectivity reached 481 mcd·m-2·lx-1 and stabilized at 342 mcd·m-2·lx-1, confirming that the formulation meets the durability requirements for high-traffic highways. The findings demonstrate that careful proportioning of functional components can balance performance and cost without relying on complex multi-additive systems.

Authors

Publication Details

Journal
Cureus Journal of Engineering.
Published
2026-11-17
DOI
https://doi.org/10.7759/s44388-026-00374-2
Primary Topic
Asphalt Pavement Performance Evaluation
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Development and Field Performance of a High-Visibility Thermoplastic Road Marking Formulation

Xiaotian Jiang
1 links
Cureus Journal of Engineering.
Asphalt Pavement Performance Evaluation
article

Development and Field Performance of a High-Visibility Thermoplastic Road Marking Formulation

Xiaotian Jiang
article en

Abstract

Thermoplastic road marking coatings are composed of a resin binder, inorganic fillers, titanium dioxide pigment, glass beads, and functional additives. The proportioning of these components determines the mechanical durability, thermal stability, and optical performance of the coating, yet systematic formulation studies remain limited. This study developed a high-visibility thermoplastic road marking formulation through a single-factor experimental approach to address the common durability problems of thermal deformation and rapid retroreflectivity loss under heavy traffic and high-temperature conditions. The investigation quantitatively evaluated the effects of premixed glass bead dosage, the mass ratio of quartz sand to calcium carbonate filler, and titanium dioxide pigment content on the mechanical strength, thermal resistance, and optical performance of the coating. The experimental results demonstrated that a premixed glass bead content ranging from 31% to 33% provided the best combination of wear resistance and compressive strength. Regarding the filler composition, a quartz sand fraction of 6% to 7% formed a rigid skeletal network that effectively improved thermal deformation resistance and maintained compressive strength at 60℃. For optical performance, a rutile titanium dioxide dosage of 4.5% to 5.5% met the luminance factor requirements while avoiding the diminishing returns caused by particle agglomeration at higher concentrations. The optimized formulation, which employed a simplified additive system consisting solely of polyethylene wax and dioctyl phthalate plasticizer, was applied in a highway maintenance project with drop-on glass beads. Six months of field tracking showed that the initial retroreflectivity reached 481 mcd·m-2·lx-1 and stabilized at 342 mcd·m-2·lx-1, confirming that the formulation meets the durability requirements for high-traffic highways. The findings demonstrate that careful proportioning of functional components can balance performance and cost without relying on complex multi-additive systems.

Cureus Journal of Engineering.
Industry, innovation and infrastructure, Sustainable cities and communities
Asphalt Pavement Performance Evaluation
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon