Statistical Analysis of the Strength of Polymer-Impregnated E-Glass Yarns Before and After Alkaline Exposure

When glass filaments are bundled as a yarn and impregnated with a polymer, the analysis of the strength distribution becomes complex, as filament load-sharing and coating efficiency govern rupture, especially under alkali attack. This study investigates the tensile strength and its statistical characteristics of acrylic-impregnated E-glass yarns, containing 4200 filaments of 17 μm in diameter and a polymer content of 17%, before and after alkaline exposure, along with the corresponding uncoated yarn. The tensile strength of the uncoated yarn is found to be lower than that estimated for a single filament, with a gradual reduction in stiffness due to progressive filament failure originating at 40% of the yarn strength. Both the uncoated and impregnated yarns exhibited Weibull strength distributions, with the latter having a substantially higher Weibull modulus. Importantly, the coating leads to yarn strength much beyond that of the greige and about 10% higher than the estimated single filament strength while maintaining the stiffness up to failure, indicating that the polymer matrix governs filament load-sharing and failure. This could be attributed to the higher Weibull modulus of the impregnated yarn (i.e., 18 for coated yarn versus 9 and 7 for the greige and single filament, respectively). The impregnated yarns were also tested after exposure to an alkaline solution with pH 13 for 7, 28, and 56 days. Such attack caused only marginal strength loss after 7 days but later reduced the mean yarn strength by 33% after 56 days. Despite such degradation, the elastic modulus, coefficient of variation of the strength, and Weibull modulus remained unchanged throughout the exposure period. The results suggest that alkaline exposure predominantly leads to propagation of existing flaws rather than introducing new, larger defects. The findings through the Weibull analysis demonstrate that polymer-impregnation of E-glass yarn increases strength, lowers variability and promotes stiffness retention until rupture. Moreover, alkaline degradation shifts the strength distribution toward lower values without substantially increasing its scatter.

Authors

Institutions

Publication Details

Journal
Textiles
Published
2026-11-16
DOI
https://doi.org/10.3390/textiles6040140
Primary Topic
Fiber-reinforced polymer composites
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Statistical Analysis of the Strength of Polymer-Impregnated E-Glass Yarns Before and After Alkaline Exposure

Ravindra Gettu, Sai Sri Kusumanchi, Sunny Raj
1 links
Textiles
Fiber-reinforced polymer composites
article

Statistical Analysis of the Strength of Polymer-Impregnated E-Glass Yarns Before and After Alkaline Exposure

Ravindra Gettu, Sai Sri Kusumanchi, Sunny Raj
article en

Abstract

When glass filaments are bundled as a yarn and impregnated with a polymer, the analysis of the strength distribution becomes complex, as filament load-sharing and coating efficiency govern rupture, especially under alkali attack. This study investigates the tensile strength and its statistical characteristics of acrylic-impregnated E-glass yarns, containing 4200 filaments of 17 μm in diameter and a polymer content of 17%, before and after alkaline exposure, along with the corresponding uncoated yarn. The tensile strength of the uncoated yarn is found to be lower than that estimated for a single filament, with a gradual reduction in stiffness due to progressive filament failure originating at 40% of the yarn strength. Both the uncoated and impregnated yarns exhibited Weibull strength distributions, with the latter having a substantially higher Weibull modulus. Importantly, the coating leads to yarn strength much beyond that of the greige and about 10% higher than the estimated single filament strength while maintaining the stiffness up to failure, indicating that the polymer matrix governs filament load-sharing and failure. This could be attributed to the higher Weibull modulus of the impregnated yarn (i.e., 18 for coated yarn versus 9 and 7 for the greige and single filament, respectively). The impregnated yarns were also tested after exposure to an alkaline solution with pH 13 for 7, 28, and 56 days. Such attack caused only marginal strength loss after 7 days but later reduced the mean yarn strength by 33% after 56 days. Despite such degradation, the elastic modulus, coefficient of variation of the strength, and Weibull modulus remained unchanged throughout the exposure period. The results suggest that alkaline exposure predominantly leads to propagation of existing flaws rather than introducing new, larger defects. The findings through the Weibull analysis demonstrate that polymer-impregnation of E-glass yarn increases strength, lowers variability and promotes stiffness retention until rupture. Moreover, alkaline degradation shifts the strength distribution toward lower values without substantially increasing its scatter.

TextilesVol. 6(4)
Indian Institute of Technology Madras (IN)
Department of Science and Technology, Ministry of Science and Technology, India
Fiber-reinforced polymer composites
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon