Mutual effects of accelerated carbonation and GGBFS stabilization on the mechanical performance and heavy‐metal immobilization of iron ore tailings

Abstract Pressurized CO 2 carbonation combined with ground granulated blast‐furnace slag (GGBFS) was evaluated as a low‐carbon strategy for valorizing iron ore tailings. Compacted tailings containing 0–9 wt % GGBFS were carbonated at 0.5–1.5 bar for 2–8 h and examined by UU triaxial testing, SEM–EDS, TGA, TCLP, and LCA. At 200 kPa confinement, untreated tailings reached 503 kPa peak deviator stress, compared with 780 kPa after carbonation alone at 1.5 bar and 1058 kPa with 9 wt % GGBFS, corresponding to increases of 55% and 110%, respectively. Surface porosity decreased from 43.3% to 28.5%, Ca content increased from 9.38 to 20.82 wt %, and TGA supported carbonate‐bearing product formation and matrix densification. The combined treatment reduced leaching of all investigated metals by 70.0–90.5% relative to untreated tailings. Under the adopted system boundary and assumptions, LCA indicated up to 75% reductions in global warming potential and energy demand relative to cement‐based stabilization.

Authors

Institutions

Publication Details

Journal
Environmental Progress & Sustainable Energy
Published
2026-11-16
DOI
https://doi.org/10.1002/ep.70812
Primary Topic
Tailings Management and Properties
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mutual effects of accelerated carbonation and GGBFS stabilization on the mechanical performance and heavy‐metal immobilization of iron ore tailings

Erol Yilmaz, Amir Hamidi, Arash Ghorbanipour
2 links
Environmental Progress & Sustainable Energy
Tailings Management and Properties
article

Mutual effects of accelerated carbonation and GGBFS stabilization on the mechanical performance and heavy‐metal immobilization of iron ore tailings

Erol Yilmaz, Amir Hamidi, Arash Ghorbanipour
article en

Abstract

Abstract Pressurized CO 2 carbonation combined with ground granulated blast‐furnace slag (GGBFS) was evaluated as a low‐carbon strategy for valorizing iron ore tailings. Compacted tailings containing 0–9 wt % GGBFS were carbonated at 0.5–1.5 bar for 2–8 h and examined by UU triaxial testing, SEM–EDS, TGA, TCLP, and LCA. At 200 kPa confinement, untreated tailings reached 503 kPa peak deviator stress, compared with 780 kPa after carbonation alone at 1.5 bar and 1058 kPa with 9 wt % GGBFS, corresponding to increases of 55% and 110%, respectively. Surface porosity decreased from 43.3% to 28.5%, Ca content increased from 9.38 to 20.82 wt %, and TGA supported carbonate‐bearing product formation and matrix densification. The combined treatment reduced leaching of all investigated metals by 70.0–90.5% relative to untreated tailings. Under the adopted system boundary and assumptions, LCA indicated up to 75% reductions in global warming potential and energy demand relative to cement‐based stabilization.

Environmental Progress & Sustainable Energy
Recep Tayyip Erdoğan University (TR), Kharazmi University (IR)
Responsible consumption and production, Climate action, Industry, innovation and infrastructure
Tailings Management and Properties
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon