A constitutive framework for fracture mode diagram of hydrogen-degraded steels: coupled void damage, quasi-cleavage, and rate-dependent transport
Hydrogen-charged steels often show quasi-cleavage (QC) near the surface and ductile dimples in the bulk. In the proposed model, void nucleation, growth, distortion, coalescence and QC compete at each material point under a single damage criterion. The QC rate law describes hydrogen-enhanced decohesion mediated by localised plasticity (HELP-mediated HEDE), driven by the Mori–Tanaka-recovered matrix stress and gated by hydrogen availability, and only QC and distortion damage are regularised non-locally. Coupled with hydrogen transport, the model is applied to X70-type smooth bars at various hydrogen concentrations and Péclet numbers ( Pe ). QC failure requires a threshold concentration, initiates at the surface and penetrates deeper as Pe decreases. With increasing hydrogen, the reduction of area at first failure falls from 84–85% to 25–26% almost independently of Pe , whereas the strain to crack 10% of the section decreases with Pe . Equal- Pe analyses coincide, and QC competes with ductile failure only through matrix-stress amplification.
Authors
- Che Zhang (ORCID: https://orcid.org/0000-0002-0987-8122)
- Rui Wang (ORCID: https://orcid.org/0000-0001-6403-2499)
- Cheng Lü (ORCID: https://orcid.org/0000-0003-2922-6962)
- Hui Wang
- Jiaqing Li
Institutions
- Nantong University (CN)
- University of Wollongong (AU)
- The University of Tokyo (JP)
- Fuzhou University (CN)
Publication Details
- Journal
- International Journal of Hydrogen Energy
- Published
- 2026-11-16
- DOI
- https://doi.org/10.1016/j.ijhydene.2026.158526
- Primary Topic
- Hydrogen embrittlement and corrosion behaviors in metals
- Type
- article
- Field-Weighted Citation Impact
- 0.00