Shear Behavior of 3D-Printed Embossed Textured Geomembrane and Geosynthetic Clay Liner Interface

The stability of waste containment facilities is critical for protecting the environment and contributing to sustainability, which is highly reliant on the interfacial strength of the composite liners consisting of a layer of geomembrane (GM) and a layer of geosynthetic clay liner (GCL). This study investigated the shear behavior of the GM–GCL interface with 3D-printed embossed textured geomembranes (3D-GMTEs) using large-scale direct shear tests under normal stresses of 100, 200, and 400 kPa. The asperity height, diameter, and spacing of the 3D-GMTEs were varied independently to evaluate their effects on interfacial shear strength. The 3D-GMTE–GCL interface showed similar overall shear stress–displacement responses to those of the commercial GMTE–GCL interface, but its large-displacement strengths were higher. The results show that, at 200 kPa, increasing asperity height from 0.5 mm to 1.0 mm increased the peak and large-displacement strengths by approximately 311% and 220%, respectively. The diameter associated with the highest peak and large-displacement strengths was 2 mm at 100 kPa and 3 mm at 200 and 400 kPa, whereas increasing asperity spacing from 4 mm to 16 mm consistently reduced shear strength. As asperity height increased from 0.5 mm to 1.5 mm, the peak and large-displacement friction angles increased from 9° and 6° to 34° and 20°, respectively. At 400 kPa, all interfaces remained compressive, with a final compression of 0.72 mm for the reference geometry. Post-shear photographs provided qualitative evidence of asperity deformation, localized penetration, fiber disturbance, bentonite extrusion, and shear striations. These findings establish a fundamental relationship between asperity-scale geometry and GMTE–GCL interface performance, providing mechanistic insights for the rational design of reliability, protecting the surrounding environment from waste contamination, and contributing to sustainability.

Authors

Institutions

Publication Details

Journal
Sustainability
Published
2026-11-16
DOI
https://doi.org/10.3390/su182211673
Primary Topic
Geotechnical Engineering and Soil Stabilization
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Shear Behavior of 3D-Printed Embossed Textured Geomembrane and Geosynthetic Clay Liner Interface

Juan Hou, Xuelei Xie, Lu Shen
1 links
Sustainability
Geotechnical Engineering and Soil Stabilization
article

Shear Behavior of 3D-Printed Embossed Textured Geomembrane and Geosynthetic Clay Liner Interface

Juan Hou, Xuelei Xie, Lu Shen
article en

Abstract

The stability of waste containment facilities is critical for protecting the environment and contributing to sustainability, which is highly reliant on the interfacial strength of the composite liners consisting of a layer of geomembrane (GM) and a layer of geosynthetic clay liner (GCL). This study investigated the shear behavior of the GM–GCL interface with 3D-printed embossed textured geomembranes (3D-GMTEs) using large-scale direct shear tests under normal stresses of 100, 200, and 400 kPa. The asperity height, diameter, and spacing of the 3D-GMTEs were varied independently to evaluate their effects on interfacial shear strength. The 3D-GMTE–GCL interface showed similar overall shear stress–displacement responses to those of the commercial GMTE–GCL interface, but its large-displacement strengths were higher. The results show that, at 200 kPa, increasing asperity height from 0.5 mm to 1.0 mm increased the peak and large-displacement strengths by approximately 311% and 220%, respectively. The diameter associated with the highest peak and large-displacement strengths was 2 mm at 100 kPa and 3 mm at 200 and 400 kPa, whereas increasing asperity spacing from 4 mm to 16 mm consistently reduced shear strength. As asperity height increased from 0.5 mm to 1.5 mm, the peak and large-displacement friction angles increased from 9° and 6° to 34° and 20°, respectively. At 400 kPa, all interfaces remained compressive, with a final compression of 0.72 mm for the reference geometry. Post-shear photographs provided qualitative evidence of asperity deformation, localized penetration, fiber disturbance, bentonite extrusion, and shear striations. These findings establish a fundamental relationship between asperity-scale geometry and GMTE–GCL interface performance, providing mechanistic insights for the rational design of reliability, protecting the surrounding environment from waste contamination, and contributing to sustainability.

SustainabilityVol. 18(22)
Shanghai University (CN), Qinghai University (CN)
National Natural Science Foundation of China, China Scholarship Council
Geotechnical Engineering and Soil Stabilization
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.