Hybrid Alkali-Activated Brick-Waste Binders: Synthesis Optimization, Mechanical Performance and Reaction Mechanisms
Brick waste from construction and demolition is predominantly crystalline and develops little strength when alkali-activated at room temperature. This study examined whether the controlled addition of Portland-composite cement (PC) can overcome this limitation. Ground brick powder was activated with NaOH and colloidal silica, and the PC/binder mass ratio (10–40 wt.%), Na2O/binder mass ratio (1.5–6.0 wt.%) and SiO2/Na2O molar ratio (0.50–1.25) were varied according to a Taguchi L16 design. PC content was the dominant factor for 7-day compressive strength, followed by the SiO2/Na2O ratio, whereas the Na2O dosage had no significant effect on strength. The mixture with the highest predicted strength within the investigated range reached 12.41 MPa at 7 days and 19.3 MPa at 90 days under ambient curing, 9.6 and 4.5 times the strength of the brick-only reference, while a low-alkali mixture (1.5 wt.% Na2O) achieved a comparable strength. Curing at 60 °C gave 17.2 MPa at 7 days. Flow was governed mainly by the Na2O dosage, and all tested hybrid pastes set much faster than the reference binders. Calorimetry, thermogravimetry and X-ray diffraction were consistent with greater reaction-product formation than in the brick-only binder. The strengths achieved point to non-structural applications, such as masonry mortars and precast elements.
Authors
- Dimitrios Kioupis (ORCID: https://orcid.org/0000-0003-3132-5919)
- EFSTRATIOS G. BADOGIANNIS (ORCID: https://orcid.org/0000-0001-5947-1331)
- Glikeria Kakali
- Anastasia Vantaraki
- Angeliki Stathi
Institutions
- National Technical University of Athens (GR)
- Merchant Marine Academy (GR)
Publication Details
- Journal
- Construction Materials
- Published
- 2026-11-16
- DOI
- https://doi.org/10.3390/constrmater6060106
- Primary Topic
- Concrete and Cement Materials Research
- Type
- article
- Field-Weighted Citation Impact
- 0.00