Selective Recovery of Lithium from Waste Lithium Aluminosilicate Glass via Mixed Sulfate Roasting and Water Leaching

Waste lithium aluminosilicate (LAS) glass is a complex secondary resource characterized by high aluminum and high silicon content, posing significant challenges for the selective recovery of lithium. Conventional recycling processes for such materials are often hindered by poor separation selectivity, complex purification steps, and high energy consumption. To address these limitations, this study proposes an integrated process comprising mixed sulfate roasting, water leaching, selective magnesium precipitation, and lithium carbonate crystallization. Under optimal conditions with a mass ratio of m(K2SO4):m(Na2SO4):m (raw material) = 0.5:0.5:1, roasting at 900 °C for 120 min resulted in the conversion of over 97% of lithium into water-soluble lithium-containing sulfate phases, while aluminum and silicon were transformed into insoluble phases, specifically KAlSi2O6 and Na (AlSi3O8). Subsequent water leaching enabled the direct separation of lithium without the use of acids or alkalis. After roasting and water leaching, a lithium leaching efficiency of 97.19% was achieved, whereas the leaching efficiencies of aluminum and silicon were both below 0.01%, demonstrating exceptional separation selectivity. Residual magnesium impurities in the lithium-bearing leachate were effectively removed via sodium hydroxide precipitation. At an optimized pH of 10.18, the magnesium removal efficiency reached 99.05%. Following purification, lithium carbonate was recovered by sodium carbonate precipitation at 95 °C for 60 min, yielding a Li2CO3 precipitation recovery of 95.33%. Based on these stages, the actual overall lithium recovery of the entire process was calculated to be 92.68%. Compared with conventional LAS-processing routes (salt roasting and acid leaching, or CaO-based calcination generating large amounts of solid waste), this process uses only deionized water for leaching, eliminating acid or alkali consumption. Relative to the conventional spodumene route (1100 °C phase transformation + acid or alkali leaching), the roasting temperature is lowered by 200 °C to 900 °C. This novel process offers a sustainable and economically viable pathway for lithium recovery from waste LAS glass, characterized by reduced energy consumption, minimized environmental impact, and enhanced resource utilization.

Authors

Institutions

Publication Details

Journal
Metals
Published
2026-11-16
DOI
https://doi.org/10.3390/met16111258
Primary Topic
Extraction and Separation Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Selective Recovery of Lithium from Waste Lithium Aluminosilicate Glass via Mixed Sulfate Roasting and Water Leaching

Jinfa Liao, Feixiong Chen, Lei Liu, Jie Liu et al.
2 links
Metals
Extraction and Separation Processes
article

Selective Recovery of Lithium from Waste Lithium Aluminosilicate Glass via Mixed Sulfate Roasting and Water Leaching

Jinfa Liao, Feixiong Chen, Lei Liu, Jie Liu, Tao Zhang, Fupeng Liu
article en

Abstract

Waste lithium aluminosilicate (LAS) glass is a complex secondary resource characterized by high aluminum and high silicon content, posing significant challenges for the selective recovery of lithium. Conventional recycling processes for such materials are often hindered by poor separation selectivity, complex purification steps, and high energy consumption. To address these limitations, this study proposes an integrated process comprising mixed sulfate roasting, water leaching, selective magnesium precipitation, and lithium carbonate crystallization. Under optimal conditions with a mass ratio of m(K2SO4):m(Na2SO4):m (raw material) = 0.5:0.5:1, roasting at 900 °C for 120 min resulted in the conversion of over 97% of lithium into water-soluble lithium-containing sulfate phases, while aluminum and silicon were transformed into insoluble phases, specifically KAlSi2O6 and Na (AlSi3O8). Subsequent water leaching enabled the direct separation of lithium without the use of acids or alkalis. After roasting and water leaching, a lithium leaching efficiency of 97.19% was achieved, whereas the leaching efficiencies of aluminum and silicon were both below 0.01%, demonstrating exceptional separation selectivity. Residual magnesium impurities in the lithium-bearing leachate were effectively removed via sodium hydroxide precipitation. At an optimized pH of 10.18, the magnesium removal efficiency reached 99.05%. Following purification, lithium carbonate was recovered by sodium carbonate precipitation at 95 °C for 60 min, yielding a Li2CO3 precipitation recovery of 95.33%. Based on these stages, the actual overall lithium recovery of the entire process was calculated to be 92.68%. Compared with conventional LAS-processing routes (salt roasting and acid leaching, or CaO-based calcination generating large amounts of solid waste), this process uses only deionized water for leaching, eliminating acid or alkali consumption. Relative to the conventional spodumene route (1100 °C phase transformation + acid or alkali leaching), the roasting temperature is lowered by 200 °C to 900 °C. This novel process offers a sustainable and economically viable pathway for lithium recovery from waste LAS glass, characterized by reduced energy consumption, minimized environmental impact, and enhanced resource utilization.

MetalsVol. 16(11)
Jiangxi University of Science and Technology (CN)
Responsible consumption and production
Extraction and Separation Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon