Experimental Investigation and Finite Element Analysis of the Cyclic Performance of Cast-in-Place Middle Slab Connections in Subway Stations
Cast-in-place middle slab connections transfer bending and shear between the slab and its supports in subway stations. Their cyclic performance depends on how the corbel and waist beam carry load as the slab deforms. A full-scale connection was tested under reversed displacement-controlled loading. Measured forces, crack patterns, and bar strains were compared with the calculated force response and damage fields. The connection exhibited good cyclic performance, with a broad post-yield resistance plateau, a mean displacement ductility coefficient of 6.48, and increasing energy dissipation over a wide displacement range. At intermediate amplitudes, repeated cycles retained most of the first-cycle resistance and dissipated energy. Damage progressed from slab cracking to concentrated flexural deformation, followed by cover spalling and longitudinal-bar fracture at large excursions. The numerical damage fields provide a qualitative indication of concentrated demand around the slab–corbel junction, consistent with the observed damage region. The findings support coordinated detailing of slab reinforcement, anchorage, corbel reinforcement, and support confinement to maintain a ductile load path.
Authors
- Qianwei Xu (ORCID: https://orcid.org/0000-0002-4833-9340)
- Guozhu Zhang
- Linhai Lu
- Jiecheng Sun
Institutions
- Tongji University (CN)
- Southeast University (CN)
Publication Details
- Journal
- Applied Sciences
- Published
- 2026-11-16
- DOI
- https://doi.org/10.3390/app162211352
- Primary Topic
- Seismic Performance and Analysis
- Type
- article
- Field-Weighted Citation Impact
- 0.00
Funders
- Department of Science and Technology of Shandong Province
- National Natural Science Foundation of China