Monomer conversion, flexural strength, fluoride release, and color stability of experimental resin composites containing bioactive glass nanoparticles: an in vitro study

Objectives This study evaluated the degree of conversion (DC), mechanical properties, fluoride release, and color stability of a newly developed ion-releasing resin composite (Thamfil) containing calcium phosphate and bioactive glass compared to commercial materials. Methods DC was measured using attenuated total reflectance Fourier-transform infrared spectroscopy ( n = 5). Biaxial flexural strength (BFS) and modulus (BFM) were tested after 24 hours of immersion in deionized water at 37°C ( n = 5). The cumulative fluoride release in deionized water for 4 weeks was also determined ( n = 4). Color stability (∆E* 00 ) was assessed after continuous immersion in deionized water or red wine at 37°C for 2 weeks ( n = 5 per solution) using an intraoral spectrophotometer. Comparisons included FiltekBulk (3M Oral Care), BeautifilBulk (Shofu), and CentionN (Ivoclar Vivadent). Results Thamfil showed significantly higher DC (74%) than other materials (46%–54%, p < 0.05). BFS was highest for FiltekBulk (232 MPa), while Thamfil (133 MPa) was comparable to CentionN (160 MPa) and BeautifilBulk (126 MPa) ( p > 0.05). BFM of Thamfil (2.6 GPa) was similar to that of BeautifilBulk (2.3 GPa) and CentionN (3.3 GPa) ( p > 0.05). The cumulative fluoride release at 28 days for Thamfil (3.3 ppm) was comparable to BeautifilBulk (3.4 ppm) but was lower than CentionN (92.3 ppm). Thamfil showed higher ∆E* 00 in water (3.6) than other materials (0.5–1.3) ( p < 0.05), but a similar color change in red wine (39.2) to that of FiltekBulk ( p > 0.05). Conclusions Thamfil exhibited high polymerization but low color stability. However, the material exhibited comparable strength and fluoride release to those of a commercial ion-releasing material (BeautifilBulk).

Authors

Institutions

Publication Details

Journal
Restorative Dentistry & Endodontics
Published
2026-11-17
DOI
https://doi.org/10.5395/rde.2026.51.e46
Primary Topic
Dental materials and restorations
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Monomer conversion, flexural strength, fluoride release, and color stability of experimental resin composites containing bioactive glass nanoparticles: an in vitro study

Piyaphong Panpisut, Parichart Naruphontjirakul, Chawal Padunglappisit, Tongjai Chotitanmapong et al.
1 links
Restorative Dentistry & Endodontics
Dental materials and restorations
article

Monomer conversion, flexural strength, fluoride release, and color stability of experimental resin composites containing bioactive glass nanoparticles: an in vitro study

Piyaphong Panpisut, Parichart Naruphontjirakul, Chawal Padunglappisit, Tongjai Chotitanmapong, Nitchakarn Leenutaphong, Wuttipong Chontanasawat, Phantira Vatthanachairoj, Linlinee Arnanthigo, Pakkapol Assawaarsu, Sawaskorn Temkitthaworn, Papawarin Amornchaiyakij
article en

Abstract

Objectives This study evaluated the degree of conversion (DC), mechanical properties, fluoride release, and color stability of a newly developed ion-releasing resin composite (Thamfil) containing calcium phosphate and bioactive glass compared to commercial materials. Methods DC was measured using attenuated total reflectance Fourier-transform infrared spectroscopy ( n = 5). Biaxial flexural strength (BFS) and modulus (BFM) were tested after 24 hours of immersion in deionized water at 37°C ( n = 5). The cumulative fluoride release in deionized water for 4 weeks was also determined ( n = 4). Color stability (∆E* 00 ) was assessed after continuous immersion in deionized water or red wine at 37°C for 2 weeks ( n = 5 per solution) using an intraoral spectrophotometer. Comparisons included FiltekBulk (3M Oral Care), BeautifilBulk (Shofu), and CentionN (Ivoclar Vivadent). Results Thamfil showed significantly higher DC (74%) than other materials (46%–54%, p < 0.05). BFS was highest for FiltekBulk (232 MPa), while Thamfil (133 MPa) was comparable to CentionN (160 MPa) and BeautifilBulk (126 MPa) ( p > 0.05). BFM of Thamfil (2.6 GPa) was similar to that of BeautifilBulk (2.3 GPa) and CentionN (3.3 GPa) ( p > 0.05). The cumulative fluoride release at 28 days for Thamfil (3.3 ppm) was comparable to BeautifilBulk (3.4 ppm) but was lower than CentionN (92.3 ppm). Thamfil showed higher ∆E* 00 in water (3.6) than other materials (0.5–1.3) ( p < 0.05), but a similar color change in red wine (39.2) to that of FiltekBulk ( p > 0.05). Conclusions Thamfil exhibited high polymerization but low color stability. However, the material exhibited comparable strength and fluoride release to those of a commercial ion-releasing material (BeautifilBulk).

Restorative Dentistry & Endodontics
Thammasat University (TH), King Mongkut's University of Technology Thonburi (TH)
Good health and well-being
Dental materials and restorations
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon