High-strength, low-thermal-conductivity porous SiOC/silica aerogel composites fabricated via precursor conversion and impregnation

Porous SiOC/silica aerogel composites were successfully fabricated through a combined route of precursor conversion, sol–gel reaction-induced phase separation, and impregnation. By varying the pyrolysis temperature, the pore structure of the SiOC matrix was tailored, which directly governed its mechanical strength. The optimal pre-impregnation properties, a compressive strength of 163.65 ± 11.39 MPa and a modulus of 5.87 ± 0.12 GPa, were achieved at 1200 °C. Subsequent silica aerogel impregnation further enhanced the compressive strength by approximately 7.9% while reducing the thermal conductivity from 0.274 to 0.261 W·m −1 ·K −1 . This work demonstrates that the synthesized composite is a promising candidate for thermal insulation applications requiring high mechanical load-bearing capacity.

Authors

Institutions

Publication Details

Journal
Advances in Applied Ceramics Structural Functional and Bioceramics
Published
2026-11-16
DOI
https://doi.org/10.1177/17436753261507817
Primary Topic
Aerogels and thermal insulation
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

High-strength, low-thermal-conductivity porous SiOC/silica aerogel composites fabricated via precursor conversion and impregnation

Yanyuan Liang, Mingwei Chen, Qiu Haipeng, Jiao Yan et al.
3 links
Advances in Applied Ceramics Structural Functional and Bioceramics
Aerogels and thermal insulation
article

High-strength, low-thermal-conductivity porous SiOC/silica aerogel composites fabricated via precursor conversion and impregnation

Yanyuan Liang, Mingwei Chen, Qiu Haipeng, Jiao Yan, Luyang Jiao, Shijian Liu
article en

Abstract

Porous SiOC/silica aerogel composites were successfully fabricated through a combined route of precursor conversion, sol–gel reaction-induced phase separation, and impregnation. By varying the pyrolysis temperature, the pore structure of the SiOC matrix was tailored, which directly governed its mechanical strength. The optimal pre-impregnation properties, a compressive strength of 163.65 ± 11.39 MPa and a modulus of 5.87 ± 0.12 GPa, were achieved at 1200 °C. Subsequent silica aerogel impregnation further enhanced the compressive strength by approximately 7.9% while reducing the thermal conductivity from 0.274 to 0.261 W·m −1 ·K −1 . This work demonstrates that the synthesized composite is a promising candidate for thermal insulation applications requiring high mechanical load-bearing capacity.

Advances in Applied Ceramics Structural Functional and Bioceramics
AviChina Industry & Technology (China) (CN), AVIC Manufacturing Technology Institute (China) (CN)
National Defense Basic Scientific Research Program of China
Industry, innovation and infrastructure
Aerogels and thermal insulation
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon