Effect of steady magnetic field on microstructure and microhardness of laser-directed energy-deposited Ti6Al4V/TiC composite coatings

Coarse microstructures, reinforcement agglomeration, and non-uniform property distribution are critical issues in laser-directed energy-deposited Ti6Al4V/TiC composite coatings. To address these issues, this study adopts a steady magnetic field with gradient intensities to assist the laser-directed energy deposition process. Ti-based composite coatings were fabricated on Ti6Al4V substrates under three laser processes with different heat inputs. Macroscopic observation, microstructural characterization, and microhardness tests were performed to investigate the coupled effects of magnetic field strength and laser heat input on coating formation quality, microstructural evolution, and microhardness. A magnetic modulation coupling coefficient K was proposed to quantitatively evaluate the modulation performance. The results show that the steady magnetic field effectively improved the macroscopic forming quality of the coatings. Surface defects decreased, and the wetting angle increased monotonically with rising magnetic field strength. The magnetic field’s modulation of microstructure and hardness was highly process-dependent. Under medium- (1,000 W, 350 mm/min, 1.2 r/min) and low-heat-input processes (800 W, 350 mm/min, 1.0 r/min), a low magnetic field of 4.07 mT yielded the optimal grain refinement and TiC dispersion uniformity. For the low-heat-input process, coating hardness first decreased slightly and then increased continuously with increasing magnetic field strength. For the medium-heat-input process, hardness increased monotonically, reaching its maximum at 12.11 mT. Under the high-heat-input process (1,200 W, 250 mm/min, 1.0 r/min), a low magnetic field aggravated microstructural coarsening, and significant strengthening was achieved only when the field strength reached 12.11 mT. The maximum coating hardness reached 1155.16 HV0.2, 50.85% higher than that of the sample without a magnetic field. The hardness evolution is governed by the combined effect of grain refinement and second-phase evolution. The proposed coupling coefficient can effectively quantify the interaction between the magnetic field and laser energy, providing a theoretical reference for optimizing steady-magnetic-field-assisted laser-directed energy deposition.

Authors

Institutions

Publication Details

Journal
Materials Science in Additive Manufacturing
Published
2026-11-16
DOI
https://doi.org/10.36922/msam026360090
Primary Topic
Surface Treatment and Coatings
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effect of steady magnetic field on microstructure and microhardness of laser-directed energy-deposited Ti6Al4V/TiC composite coatings

Chao Zeng, Quanou Yang, Qingmei Qian
3 links
Materials Science in Additive Manufacturing
Surface Treatment and Coatings
article

Effect of steady magnetic field on microstructure and microhardness of laser-directed energy-deposited Ti6Al4V/TiC composite coatings

Chao Zeng, Quanou Yang, Qingmei Qian
article en

Abstract

Coarse microstructures, reinforcement agglomeration, and non-uniform property distribution are critical issues in laser-directed energy-deposited Ti6Al4V/TiC composite coatings. To address these issues, this study adopts a steady magnetic field with gradient intensities to assist the laser-directed energy deposition process. Ti-based composite coatings were fabricated on Ti6Al4V substrates under three laser processes with different heat inputs. Macroscopic observation, microstructural characterization, and microhardness tests were performed to investigate the coupled effects of magnetic field strength and laser heat input on coating formation quality, microstructural evolution, and microhardness. A magnetic modulation coupling coefficient K was proposed to quantitatively evaluate the modulation performance. The results show that the steady magnetic field effectively improved the macroscopic forming quality of the coatings. Surface defects decreased, and the wetting angle increased monotonically with rising magnetic field strength. The magnetic field’s modulation of microstructure and hardness was highly process-dependent. Under medium- (1,000 W, 350 mm/min, 1.2 r/min) and low-heat-input processes (800 W, 350 mm/min, 1.0 r/min), a low magnetic field of 4.07 mT yielded the optimal grain refinement and TiC dispersion uniformity. For the low-heat-input process, coating hardness first decreased slightly and then increased continuously with increasing magnetic field strength. For the medium-heat-input process, hardness increased monotonically, reaching its maximum at 12.11 mT. Under the high-heat-input process (1,200 W, 250 mm/min, 1.0 r/min), a low magnetic field aggravated microstructural coarsening, and significant strengthening was achieved only when the field strength reached 12.11 mT. The maximum coating hardness reached 1155.16 HV0.2, 50.85% higher than that of the sample without a magnetic field. The hardness evolution is governed by the combined effect of grain refinement and second-phase evolution. The proposed coupling coefficient can effectively quantify the interaction between the magnetic field and laser energy, providing a theoretical reference for optimizing steady-magnetic-field-assisted laser-directed energy deposition.

Materials Science in Additive ManufacturingVol. 0(0)
Guizhou Normal University (CN), Guizhou Institute of Technology (CN)
Surface Treatment and Coatings
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon